1. Introduction
Stainless steel investment casting, also known as precision casting or lost wax casting, is a highly precise and versatile manufacturing method used to produce complex, high-performance components with tight tolerances and excellent surface finishes.
It plays a critical role in modern industrial applications where dimensional accuracy, material integrity, and corrosion resistance are essential.
As demand for lightweight, durable, and intricately shaped parts continues to grow in industries like aerospace, medical, petrochemical, and food processing, stainless steel investment casting has become increasingly valuable.
This process allows manufacturers to create near-net-shape stainless steel parts while minimizing machining, material waste, and assembly complexity.
2. What Is Investment Casting?
Investment casting—also known as lost‑wax or precision casting—is a metal‑forming process in which a disposable wax pattern is surrounded by a multi‑layered ceramic shell.
Once the shell hardens, the wax is melted out (“lost wax”), leaving a precise cavity into which molten metal is poured.
After solidification, the ceramic shell is broken away to reveal a metal part that faithfully replicates the original wax geometry.

3. Why Use Stainless Steel for Investment Casting?
Stainless steel combines exceptional mechanical performance, corrosion resistance, and aesthetic qualities, making it one of the most versatile and reliable materials for precision investment casting.
Outstanding Corrosion Resistance
- Passive Oxide Layer: All stainless steels form a thin, self‑healing chromium‑oxide surface layer that prevents rust and staining even in harsh environments.
- Pitting Resistance: Grades such as 316L and duplex 2205 exhibit high pitting resistance equivalent numbers (PREN) of ≥25, ensuring long service life in chloride‑rich media (e.g., seawater, brine).
- Chemical Compatibility: Resistant to a broad pH range (2–13), allowing use in chemical processing, food and beverage, and pharmaceutical applications without special coatings.
High Strength and Toughness
- Wide Strength Spectrum:
-
- Austenitic grades (304L, 316L): tensile strength 480–600 MPa; yield strength 200–300 MPa.
- Precipitation‑hardening alloys (17‑4PH): tensile strength up to 1,300 MPa after aging treatment.
- Martensitic grades (410, 420): can be heat‑treated to achieve yield strengths of 800 MPa or more.
- Excellent Toughness: Even in cryogenic or sub‑zero applications, austenitic stainless steels maintain impact toughness above 80 J at –196 °C.
Precision Casting Compatibility
- Fluidity and Melting Range: Stainless steels melt between 1,350 °C and 1,500 °C, providing a stable pouring window that works seamlessly with ceramic shell materials.
- Dimensional Accuracy: Achieves tolerances as tight as ±0.1 mm per 100 mm of nominal dimension, ideal for components requiring precise fits or intricate features.
- Surface Finish: Typical as‑cast finishes reach Ra 1.6–3.2 μm, reducing or eliminating the need for secondary polishing.
4. Step‑by‑Step Process of Stainless Steel Investment Casting
The investment‑casting workflow consists of six major stages, each carefully controlled to ensure dimensional accuracy, surface quality, and metallurgical integrity.
4.1 Wax Pattern Creation
Die Design & Fabrication
- Precision steel dies are CNC‑milled to mirror the final part geometry, accounting for shrinkage (typically 1.5–2 % for stainless steel).
Wax Injection
- Molten wax (paraffin blends with plasticizers) is injected under pressure (4–6 bar) into the die, filling cavities in under 2 seconds.
- Target dimensional variation: ±0.03 mm per 25 mm.

Pattern Quality Check
- Visual inspection for voids, flash, or knit lines.
- Weight verification: each pattern’s mass is recorded to track yield and process consistency.
4.2 Assembly of Wax Patterns
Pattern Treeing
- Individual wax patterns are “grafted” onto a central wax sprue bar to form a tree, optimizing metal feed and minimizing turbulence.
- Typical tree sizes: 10–50 patterns, depending on part size and furnace capacity.

Gate and Runner Design
- Gate cross‑sections sized to balance fill speed against turbulence (aiming for Reynolds numbers below 500).
- Hot‑tap gates or daily‑flared gates reduce turbulence and air entrapment.
4.3 Shell Building (Ceramic Slurry and Stucco)
First Dipping (Prime Coat)
- Fine refractory slurry (particle size 5–10 µm) coats the wax tree to capture fine detail.

Stucco Application
- Silica or zircon sand (40–80 µm) is stuccoed onto the wet prime coat for reinforcement.
Subsequent Coats
- Alternate slurry and stucco for 5–8 total layers, building shell thickness to 6–10 mm.
- Drying time between coats: 15–30 minutes at 20–25 °C and 40–60 % relative humidity.
Final Coating
- A coarser outer layer (150–250 µm particles) provides mechanical protection during handling and pouring.
4.4 Dewaxing (Lost‑Wax)
Autoclave Dewax
- Rapid steam cycle at 120–150 °C and 2–5 bar pressure for 1–2 minutes to melt out the bulk of wax.
Oven Bake‑out
- Shells are transferred to an oven at 200–250 °C for 2–4 hours to remove residual wax and moisture.
Wax Recovery
- Melted wax is collected, filtered, and recycled back into the wax injection system, achieving over 95% reuse.
4.5 Preheating and Pouring Molten Stainless Steel
Shell Preheating
- Shell assemblies are baked at 1,000–1,200 °C for 1–3 hours to sinter the ceramic, drive off moisture, and reduce thermal shock.
Melting Furnace
- Induction or electric‑arc furnaces melt stainless charge metal to 1,400–1,550 °C, depending on alloy (e.g., 316L at ~1,450 °C).
Pouring
- Gravity pour, vacuum assist, or low‑pressure techniques fill molds at controlled rates (20–50 cm/s mold velocity) to minimize turbulence.
- Typical pour weight per shell: 10–250 kg of molten metal.

4.6 Shell Removal, Finishing
Once the stainless steel has fully solidified, the ceramic shell is removed through mechanical methods such as sandblasting, water jetting, or vibratory finishing.
In some cases, chemical dissolution may be used for intricate geometries.
After shell removal, the casting proceeds to finishing operations, which typically include removal of the sprue system, surface grinding, and polishing to achieve the desired surface quality.

Heat treatment may be applied to enhance mechanical properties such as strength, hardness, or corrosion resistance, depending on the alloy used.
Precision CNC machining is then employed to meet tight dimensional tolerances, especially on critical surfaces or mating interfaces.
5. Technical Advantages of Stainless Steel Investment Casting
Stainless steel investment casting offers a unique combination of precision, performance, and economy. Below are its principal technical advantages:

Exceptional Dimensional Accuracy
- Typical tolerances of ±0.1 mm per 100 mm of nominal dimension enable net‑shape parts that require minimal or no secondary machining.
- Consistent pattern replication and controlled shell thickness ensure repeatability across production runs.
Superior Surface Finish
- As‑cast surface roughness in the range of Ra 1.6–3.2 μm yields smooth components ready for service or light polishing.
- Fine ceramic prime coats capture intricate details and sharp edges, reducing post‑cast grinding and buffing.
Complex Geometry Capability
- Ability to produce thin walls down to 0.6 mm, internal cavities, undercuts, and negative drafts without cores.
- Facilitates consolidation of multiple parts or features into a single casting, reducing assembly steps and potential leak paths.
High Material Utilization and Yield
- Wax patterns and ceramic shells are fully reclaimable, with wax reuse rates exceeding 95 %.
- Typical metal yield of 85–95 % minimizes scrap compared to subtractive processes.
Broad Alloy Compatibility
- Successfully cast a wide spectrum of stainless grades—from 304/316 austenitics to 17‑4PH precipitation‑hardening and duplex 2205—each delivering tailored corrosion resistance, strength, and toughness.
- Uniform microstructure and controlled cooling prevent segregation, ensuring consistent mechanical properties.
Cost‑Effectiveness in Medium to High Volumes
- Tooling costs (wax dies and ceramic pattern tools) are amortized over production runs of hundreds to tens of thousands of parts, driving per‑part costs below those of machining from bar stock.
- Reduced secondary operations (welding, assembly, extensive machining) further lower total manufacturing expenses.
Shorter Lead Times for Complex Parts
- From CAD approval to first production castings in as little as 4–6 weeks, outpacing custom machining or forging for geometrically intricate components.
- Automated shell‑building and dewaxing systems support rapid, repeatable cycle times.
Enhanced Mechanical Performance
- Near‑net shape pouring minimizes stress concentrators and machining‑induced work hardening, improving fatigue life.
- Optionally combined with heat treatments (solution annealing, aging) to fine‑tune hardness, yield strength, and toughness.
6. Design Guidelines for Stainless Steel Investment Castings
When designing parts for stainless steel investment casting, following proven guidelines ensures reliable mold filling, sound metallurgy, and minimal post‑cast refinement.
| Design Feature | Recommendation | Rationale |
| Wall Thickness | 1.0 – 12 mm; maintain variation ≤ 2:1 ratio | Promotes uniform cooling, reduces porosity |
| Draft Angles | ≥ 1° per side for vertical walls; ≥ 2° for fine detail | Eases shell removal, prevents damage |
| Fillet Radii | Internal ≥ 0.5 mm; external ≥ 1.0 mm | Enhances metal flow, reduces stress risers |
| Undercuts | Avoid when possible; otherwise use collapsible cores or removable inserts | Simplifies mold construction, reduces defects |
| Tolerance Grades | ISO 8062 CT5–CT7 for as‑cast features | CT5 (fine): ±0.05 mm; CT7 (standard): ±0.20 mm |
| Surface Finish | Ra 1.6–3.2 μm achievable; specify critical areas if finer finish is needed | Allows consolidation of finish and casting processes |
| Ribs & Bosses | Width ≤ 3× thickness; height ≤ 4× thickness; add radii at bases | Prevents hot spots and insufficient fill |
| Gating & Risers | Place gates at thick sections; risers sized to feed shrinkage | Controls feed direction, avoids shrinkage porosity |
| Coring & Holes | Use ceramic cores for internal features; holes ≥ 3 mm | Ensures accuracy of internal passages |
| Directional Solidification | Design solidification paths toward risers | Minimizes trapped liquid and porosity |
7. Common Stainless Steel Grades in Investment Casting
Stainless steel investment casting supports a wide range of alloy grades to meet diverse application demands across industries.

Each grade offers a unique combination of mechanical properties, corrosion resistance, and heat treatment capabilities.
| Grade | Equivalent Designation | Yield Strength (MPa) | Tensile Strength (MPa) | Pitting Resistance (PREN) | Typical Uses |
| 304 | CF8 | 215 | 505 | 18 | Food equipment, architectural trim |
| 316 | CF8M | 205 | 515 | 24 | Pump bodies, valves, marine components |
| 304L | CF3 | 215 | 505 | 18 | Chemical processing, low‑carbon applications |
| 316L | CF3M | 205 | 515 | 24 | Pharmaceutical, food‑grade equipment |
| 410 | — | 415 | 530 | 12 | Valves, shafts, fasteners |
| 420 | — | 450 | 655 | 14 | Cutlery, wear parts, tooling |
| 17‑4PH | — | 1,035 (H900) | 1,150 | 20 | Aerospace fittings, high‑stress components |
| 2205 | — | 450 | 620 | 32 | Oil & gas fittings, chemical processing |
8. Post-Casting Processes and Finishing Options
Post-casting operations are essential in transforming a raw stainless steel investment casting into a high-performance, precision component.
These processes improve dimensional accuracy, surface quality, mechanical properties, and ensure that the casting meets functional and regulatory requirements.
Heat Treatment
Heat treatment is often applied to stainless steel castings to improve strength, hardness, ductility, and corrosion resistance. The specific treatment depends on the alloy type:
- Austenitic Stainless Steels (e.g., 304, 316):
-
- Solution Annealing (1,040–1,120 °C): Dissolves chromium carbides, refines grain structure, and improves corrosion resistance.
- Rapid Quenching: Prevents sensitization and intergranular corrosion.
- Martensitic Stainless Steels (e.g., 410, 420):
-
- Hardening and Tempering (950–1,050 °C): Increases hardness and tensile strength.
- Tempering: Adjusts toughness and reduces brittleness after hardening.
- Precipitation-Hardening Steels (e.g., 17-4PH):
-
- Aging Treatment (e.g., H900, H1025): Improves yield strength and hardness via controlled precipitation of copper-rich phases.
Surface Treatments
Surface finishing enhances the appearance, cleanliness, and corrosion resistance of the casting. Common treatments include:
- Pickling
-
- Removes surface oxides and scale using acid solutions (typically nitric and hydrofluoric acids).
- Prepares the casting for passivation or electropolishing.
- Passivation
-
- Enhances corrosion resistance by forming a stable chromium oxide layer.
- Typically done using nitric acid or citric acid baths.
-
- Anodic dissolution process that smooths and brightens the surface by removing micro-roughness.
- Ideal for sanitary, medical, and food-grade applications.
- Shot Blasting / Sand Blasting
-
- Mechanically removes ceramic shell residue, oxidation, and surface defects.
- Commonly used as a pre-finish step before polishing or coating.
CNC Machining and Dimensional Finishing
Though investment casting achieves near-net-shape precision, some critical surfaces or tolerances may require post-machining.

- CNC Milling / Turning
-
- Used to achieve tight tolerances (e.g., ±0.01 mm) and precision surface finishes on threads, bores, or sealing faces.
- Especially important for mating parts or assemblies.
- Grinding & Polishing
-
- Applied to improve aesthetics, flatness, or prepare parts for plating or welding.
- Mirror or satin finishes can be achieved depending on requirements.
Inspection and Quality Control
After all finishing processes, castings undergo rigorous inspection to ensure conformance with specifications and reliability standards.
- Dimensional Inspection
-
- Tools: CMM (Coordinate Measuring Machines), digital calipers, gauges
- Checks critical tolerances, concentricity, and geometry.
- Non-Destructive Testing (NDT)
-
- Visual Inspection (VT): Surface flaws and defects
- Dye Penetrant Testing (PT): Surface cracks and porosity
- Radiographic Testing (RT): Internal voids and inclusions
- Ultrasonic Testing (UT): Subsurface flaws in thicker sections
- Magnetic Particle Testing (MT): For ferromagnetic martensitic grades
- Mechanical Property Testing (if required)
-
- Tensile, impact, hardness, and elongation testing according to ASTM standards.
9. Applications of Stainless Steel Investment Castings
Stainless steel investment castings are used across a wide range of industries where precision, durability, and corrosion resistance are critical.
The ability to produce complex shapes with tight tolerances and excellent surface finish makes this process especially valuable for high-performance components.

Aerospace Industry
- Turbine blades
- Engine housings
- Fuel system components
- Landing gear brackets
Why Investment Casting?
Stainless steel castings in aerospace must withstand high temperatures, mechanical stress, and corrosive environments.
Investment casting enables the production of lightweight, complex geometries with minimal post-machining, crucial for performance and fuel efficiency.
Medical and Dental Industry
- Surgical instruments
- Orthopedic implants (hip stems, bone screws)
- Dental devices and brackets
- Diagnostic equipment parts
Why Stainless Steel Investment Casting?
Medical-grade stainless steels like 316L and 17-4PH provide biocompatibility and sterilization resistance.
Investment casting allows intricate, hygienic, and repeatable parts required in medical settings.
Automotive Industry
- Turbocharger impellers
- Exhaust manifolds
- Sensor housings
- Gearbox components
Why Investment Casting?
In high-performance vehicles, precision-cast stainless steel parts offer weight savings, heat resistance, and strength.
Investment casting is ideal for low to mid-volume production of complex drivetrain or engine parts.
Food and Beverage Industry
- Pump housings
- Sanitary valves
- Pipe fittings
- Mixer blades
Why Investment Casting Stainless Steel?
Grades such as 304 and 316L are widely used due to their corrosion resistance and hygienic properties.
Investment casting produces smooth, crevice-free surfaces that are easy to clean and comply with food safety standards.
Marine and Offshore Applications
- Propellers and impellers
- Couplings and flanges
- Pump bodies
- Anchor brackets
Why Investment Casting?
Marine environments are highly corrosive, especially with saltwater exposure.
Stainless grades like 316 and duplex 2205 offer excellent resistance to pitting, crevice corrosion, and stress corrosion cracking.
Oil, Gas, and Chemical Processing
- Valve bodies
- Sealing rings
- Pump components
- Heat exchanger parts
Why Investment Casting Stainless Steel?
Components in oil & gas or chemical plants must handle pressure, temperature fluctuations, and aggressive media.
Duplex and precipitation-hardening stainless steels provide the required mechanical and corrosion resistance, while investment casting ensures dimensional accuracy and integrity.
Defense and Firearms
- Trigger components
- Barrel extensions
- Optics mounts
- Weapon housings
Why Stainless Steel Investment Casting?
Defense-grade components benefit from stainless steel’s strength and wear resistance. Investment casting supports the precision needed for moving parts and safety-critical assemblies.
10. Investment Casting vs. Other Stainless Steel Manufacturing Methods
While investment casting offers numerous advantages for producing high-quality stainless steel components, it’s important to understand how it compares with other common manufacturing methods.
★ = Poor / Low ★★★★★ = Excellent / High
| Criteria | Investment Casting | Sand Casting | Forging | CNC Machining | Die Casting(mainly non-ferrous) |
| Dimensional Accuracy | ★★★★☆ (±0.1 mm) | ★★☆☆☆ (±1.0 mm) | ★★★★☆ (±0.3 mm) | ★★★★★ (±0.01 mm) | ★★★★☆ (±0.2 mm) |
| Surface Finish (Ra) | ★★★★☆ (1.6–3.2 μm) | ★★☆☆☆ (6.3–25 μm) | ★★☆☆☆ (3.2–12.5 μm) | ★★★★★ (<1.6 μm) | ★★★★☆ (1.6–3.2 μm) |
| Tooling Cost | Medium | Low | High | Very Low (per unit) | Very High |
| Production Volume Suitability | Medium–High | Low–Medium | Medium–High | Low–Medium | Very High |
| Complex Geometry | ★★★★★ | ★★☆☆☆ | ★☆☆☆☆ | ★★★★★ | ★★★☆☆ |
| Material Yield | Medium–High | Low | Very High | Low (high waste) | High |
| Part Size Flexibility | Small–Medium | Medium–Large | Small–Very Large | Small–Medium | Small–Medium |
| Strength of Final Part | High | Medium | Very High | High | Medium |
| Lead Time | Medium | Short | Long | Medium | Long |
| Best For | Precision, complex parts | Large, simple shapes | High-strength applications | Prototypes, fine tolerances | Mass production of small components |
| Typical Applications | Aerospace, medical, valves | Pump housings, frames | Shafts, gears, flanges | Mold bases, custom fixtures | Automotive housings, appliance parts |
11. Challenges and Limitations of Investment Casting Stainless Steel
- Porosity Control: Requires optimized gating and solidification.
- Size Constraints: Generally up to 1 m in dimension; larger parts may need segmentation.
- Lead Time: 4–6 weeks from tooling to finished parts—longer than some rapid prototyping methods.
- Cost of Tooling: Initial wax die investment (~USD 3,000–5,000 per cavity) can be prohibitive for very low volumes.
12. Choosing a Stainless Steel Investment Casting Supplier—LangHe Industry
When selecting a partner, consider:
- Technical Expertise: Experience with your required grades and tolerances.
- Quality Systems: ISO 9001, AS 9100 (aerospace), ISO 13485 (medical).
- Capacity & Scalability: Ability to ramp from prototypes to tens of thousands of parts.
- Supply Chain Transparency: Traceability of raw materials and certification.
- Value‑Added Services: In‑house machining, heat treatment, finishing, and inspection.
LangHe distinguishes itself with over 20 years in stainless steel investment casting, in‑house tool making, and full turnkey capabilities, ensuring single‑source accountability and rapid response from design to production.
13. Conclusion
Stainless steel investment casting stands at the nexus of precision engineering and material science, offering unmatched freedom in design, high accuracy, and repeatable quality.
Whether you’re developing critical aerospace components or high‑precision medical instruments, the process delivers superior surface finish, mechanical performance, and cost efficiency at scale.
FAQs
What is the tolerance of stainless steel investment castings?
Typically ±0.1 mm per 100 mm of nominal dimension (ISO 8062 CT5–CT7), with tighter tolerances achievable via post‑machining.
What is the difference between investment casting and sand casting?
Investment casting yields finer detail (Ra 1.6–3.2 μm vs. Ra 6.3–12.5 μm), tighter tolerances (±0.1 mm vs. ±0.5 mm), and supports more complex geometries, whereas sand casting is more economical for very large parts or low‑precision applications.
Can 316 stainless steel be investment cast?
Yes—grade 316L is one of the most common stainless alloys for investment casting, offering excellent corrosion resistance and good mechanical properties.
How does investment casting improve part performance?
By minimizing machining (reducing stress concentrators), ensuring uniform microstructure, and achieving high surface finish, investment casting enhances fatigue life, dimensional stability, and aesthetic appeal.