ʻO keʻano o ke keleawe keleawe: 'Ikeʻike, Nā mea nui, a me na noi noi

Papa o nāʻikepili Hōʻike

1. Hōʻikeʻike

'Ōlelo ʻO keʻano o ke keleawe keleawe he waiwai waiwai e komo ana i konaʻano i ka hoʻoleiʻana, Welding, mohaihala, a me nā wela wela.

ʻAʻole like me nā metala maʻemaʻe, ʻO ke Kahu nui a hoʻohemo melū ma mua o kahi wela, ma waena 880 ° C (1,616 ° F) and 1,095 ° C (2,003 ° F), Ke hilinaʻi nei i ka hoʻohuiʻana a me nā'āpana alloying e like me zinc, alakaʻi, kū, nickel, a me ka aluminum.

ʻO ka mana kūpono o kēia neʻeʻana o kēiaʻano papa hana koʻikoʻi no nā noiʻoihanaʻoihana: e hōʻoia ia i ka hoʻopiha pihaʻana, ho'ēmi i nā mososity a me ka huki wela, mālama i nā waiwai mechanins, a pale aku i nā vulatinization zinc.

ʻO nā mea liʻiliʻi liʻiliʻi mai ka puka aniani o ke aniani hiki ke hōʻemi nui i ka hāʻawiʻana a me ka maikaʻi huahana.

Ka hoʻomaopopoʻana i nā mea i manaʻoʻia i keʻano o keʻano o keʻano keleawe, moloka, ka hoʻoiliʻana i ka mōʻaukala, a me nā kūlana kūlohelohe.

E hiki i nā mea hana hana e hoʻomaikaʻi i ka hana, E hōʻemi i nā hemahema, a loaʻa i nā hopena kūlike i nā noi noi mai nā mea hana o nā kaʻa kaʻa i nā mea kani i nā mea kani.

2. He keleawe (ka hoʻonohonohoʻana a me ka heluʻana)

keleawe E hōʻike ana i nā alloys e like me nā mea nui keleawe (Cu) and zinc (Zn).

E ka hoʻololiʻana i ka cu: Zn ratio a hoʻohui i nā helu liʻiliʻi o nā mea'ē aʻe, he ākea ākea o ka mīkini, Kuupuiawi, a hiki i nā hiʻohiʻona thermal ke hana.

Keleawe keleawe keleawe
Keleawe keleawe keleawe

Nā papa maʻamau:

  • Aphaila (a) Nā kihaia - cu-waiwai (maʻamau a hiki i ~ 35 wt% zn). ʻO ke alo o ke alo o ke alo (Fcc) Paʻa paʻa. Maikaʻi maikaʻi a me ka formability.
  • Alma-Beta (a + b) Nā kihaia - moderate zn (~ 35-45 wt%), duplex molstructure e hoʻonui ana i ka ikaika a me ka paʻakikī akā hōʻemi i ke anuanu maloʻo.
  • ʻO Zinc kiʻekiʻe a me nā lāhina kūikawā - kiʻekiʻe zn a iʻole nā ​​mea nui'ē aʻe (AL, I, Mn, Sno, Pb) Hoʻololiʻo Alter Phase eqilibria a me ka hoʻomālamalama / hoʻoponopono pono.

ʻO kēia mau mea e wehe ai i ke kumu o ke kumu o keʻano o keʻano o keʻano: ʻAʻole like me nā metala maʻemaʻe, ʻaʻole e hoʻokaʻawaleʻia nā alloys ma kahi mahana hoʻokahi akā ma luna o ke kikowaena ma waena o ka solidus a me nā laina wai e kū ana ma luna o ke kiʻi kiʻi.

3. ʻO nā'ōnaehana helu keleawe a me nā'ōnaehana maʻamau

Ma lalo iho he mau meaʻenehanaʻenehana no nā helu keleawe maʻamau a me nā helu.

Keleawe keleawe
Keleawe keleawe

ʻO kēia mau waiwai he hana maʻamau maʻamau i hoʻohanaʻia no ka hoʻolālāʻana no ke kaʻina hana a hōʻoiaʻia e kū'ē i nā palapala hōʻoia, nā mea hāʻawi waiwai, a iʻole ka nānāʻana i ka hana loiloi no ka hana no ka hana koʻikoʻi.

Alloy / ohana ʻO nā mea maʻamau (° C / ° F) ʻO ka wai maʻamau (° C / ° F) Nā memo
ʻO ke keleawe melemele gula (hui hui maʻamau) ~ 900 ° C / 1,652 ° F ~ 940 ° C / 1,724 ° F Keleawe oka; maʻalahi e hoʻolei a me ka mīkini.
C26000 (Keleawe cretridge, 70Me -30zn) ~ 910-920 ° C / 1,670-1,688 ° F ~ 954-965 ° C / 1,750-1,769 ° F Maikaʻi loa; i hoʻohana nuiʻia ma ka pepa a me ka tube.
C36000 (ʻO ke keleawe manuahi manuahi, PB-Nahu) ~ 885-890 ° C / 1,625-1,634 ° F ~ 900 ° C / 1,652 ° F ʻO ka machiniblibility; ʻO ka puka aniani marrower.
C23000 (Keka ulaula ulaula, ~ 85co-15Zn) ~ 990 ° C / 1,814 ° F ~ 1,025 ° C / 1,877 ° F ʻO ke keleawe kiʻekiʻe-CU "CU"; E pili anaʻo Melts i ke keleawe maʻemaʻe.
C46400 (Nāʻili manu, Cu -zn -sn) ~ 888 ° C / 1,630 ° F ~ 899 ° C / 1,650 ° F Pale aku i keʻano o ke kai; 'Ōpū i lalo o keʻano.
C75200 (Nickel kālā 65-18-17) ~ 1,070 ° C / 1,958 ° F ~ 1,095 ° C / 2,003 ° F Cu–Zn–Ni alloy; ʻO ke kiʻekiʻe kiʻekiʻe o ka menting ma muli o nā manaʻo ni; waiwai no ka ikaika a me keʻano kālā likeʻole.

4. ʻO nā kumu nui e hoʻolauna ana i keʻano o ke aniani o ke keleawe

Pehea nā mea e hoʻololi ai i nā mea i hoʻololiʻia i ke keleawe o ke keleawe

Mua Malting Point (° C / ° F) Hopena ma keʻano o keʻano o ke keleawe keleawe Nā hopena kūponoʻole
Zinc (Zn) 419 ° C / 786 ° F ʻO ka haʻahaʻa haʻahaʻa a me nā mea e pili ana i ka waihoʻoluʻu a me ka waihoʻoluʻu; ʻoi aku ka nui o nā zn e lele ana (A → F Phase Transitions). Hoʻomaikaʻi i ka hale noho; Hoʻonui loaʻo Zn i ka hopena o ka segregation a me Zinc i ka wā o ka holoiʻana.
Alakaʻi (Pb) 327 ° C / 621 ° F ʻAʻole e hoʻokaʻawale i ka cu-zn matrix; nāʻano e hoʻokaʻawale i nā manaʻo haʻahaʻa haʻahaʻa haʻahaʻa. Hoʻonui i ka manchinebility; Akā e hōʻeha i ka pōkole wela i ka ulding / brazing a me nā hopohopo olakino.
Kū (Sno) 232 ° C / 450 ° F E hoʻolōʻihi i ka laulā o ka hoʻokaʻawaleʻana; hoʻomaikaʻi i ke kūpaʻa o ka α-phase a me ke kū'ēʻana. Hoʻohanaʻia i loko o ka naval a me nā keleaweʻulaʻula; ʻO nā pale pale dezincification akā e koi i nā kiʻekiʻe o ke kaʻina hana kiʻekiʻe.
Nickel (I) 1,455 ° C / 2,651 ° F E hāpai i ka paʻa a me ka wai; ʻO nā mea hoʻoikaika CU-ZN Matrix; stabilizes i nā pae kiʻekiʻe kiʻekiʻe. E hana i nā mea nānā nickel (E.g., C75200) me nā kiʻekiʻe kiʻekiʻe e hoʻomaʻemaʻe ai a hoʻomaikaʻi i ka ikaika.
Aluminum (AL)
660 ° C / 1,220 ° F E hoʻohuli i ka hoʻonuiʻana i ka lewa; Hoʻolako i ka hoʻokumuʻana ma mua; hoʻomaikaʻi i ka paleʻana i ka oxidation. Hoʻohanaʻia ma nā keleawe aluminum no ka lawelawe o ke kai; pono i ke kiʻekiʻe kiʻekiʻe i ka wā o ke kauʻana.
Mang kāne (Mn) 1,246 ° C / 2,275 ° F E hōʻoluʻolu i nā microstructure; hoʻonui liʻiliʻi ma ka neʻeʻana o ka mīkini; E hana i nā'āpanaʻelua-phase. Hoʻomaikaʻi i ka ikaika a me ka paʻakikī; Hoʻopili i nā pale pale.
'Eron (Lia) 1,538 ° C / 2,800 ° F Nā mea kau palena; E hoʻolōʻihi i ka laulā o ka hoʻokaʻawaleʻana; hiki ke hana e like me ka nuclent i ka wā hoʻoponopono. Hoʻohui i ka ikaika akā hiki ke hoʻopiʻi i ka hoʻoleiʻana ma muli o nā invusions.
Silikino (A) 1,414 ° C / 2,577 ° F Hana nui e like me ka deoxidizer; ʻO ka hopena kūpono kūpono i ka hoʻohaʻahaʻaʻana i nāʻano o ka hoʻomehanaʻana akā e hoʻololi ana i ka hana oxide. Hoʻomaikaʻi i ke kani a me keʻano o ka wai; Kōkua i ka mālama ponoʻana.

Nā Moku'āina Microstructural (Ka nui o ka palaoa, Ka pae pahele)

ʻO keʻano o ke keleawe o ke keleawe he mea paʻakikī loa i kona microstructure as-solset, ʻOiai ua liʻiliʻi loa kēia hopena ma mua o ka hoʻopiliʻana:

  • Ka nui o ka palaoa: Keleawe maikaʻi (palaoa palaoa <10 }m) he solidus ~ 5-10 ° C i lalo ma lalo o ke keleawe i hoʻopaʻaʻia (>50 }m).
    Loaʻa nā momona maikaʻi i nā palena nui, kahi e wikiwiki ai ka diffusican ma kahi o kēia e hoʻololi nei i nā haʻahaʻa haʻahaʻa.
  • Phase segregeation: I loko o + s keleawe (E.g., C27200), ʻO ka hoʻokaʻawaleʻana i ka hana (E.g., β-phase clusters) hana i nā wahi i lalo.
    β-nā kumu nui o ka ult (at ~ 980 ° C), ʻOiai e hoʻomau anaʻo α-phase ke hoʻomau a hiki i ke ~ 1050 ° C, ka hoʻonuiʻana i keʻano o ka hanaʻana ma ka papa hana ma mua o 10-20 ° C.

Hōʻike Hōʻailona: ʻO ke keleawe anuanu (E.g., huki keleawe keleawe) Loaʻa i kahiʻano nui o ka palaoa nui ma mua o ke keleawe.

I ka wā e hana ai i ke anuanu-hana c26000 keleawe, Hoʻomaka ka hoʻololiʻana ma ka 1040 ° C (vsa. 1050° C no ka laweʻana iā C26000), koi ana i nā haʻahaʻa haʻahaʻa haʻahaʻa e pale ai i ka hoʻokaʻawaleʻana.

Ka hoʻoiliʻana i ka mōʻaukala (Kauhi, Welding, ʻO ka hana wela)

Ke hoʻololi neiʻo Thermal i ka hoʻomehanaʻana o ke keleawe o ke keleawe ma ka hoʻololiʻana i konaʻano chemika a iʻole nā ​​microstructural:

  • Zinc collatinization (WELDING / Kāwili): ʻO Zinc kahi wahi haʻahaʻa haʻahaʻa haʻahaʻa (907° C), No laila ke kalaʻana i ke keleawe ma luna o 950 ° C kumu kumuʻo Zinc Vapor (1-3 wt% i hoʻokahi hola ma 1000 ° C).
    Hoʻonui kēia i nāʻike keleawe, e ala ana i ka haunaele-e.g., C36000 keleawe me 3% Ua loaʻa iā Zinc ka nalowale i kahi wai o 960 ° C (vsa. 940° C no ka uku kālāʻole).
  • ʻO ka hana wela (Hoʻoholo hōʻoluʻolu): ʻO ke keleawe ma kahi o 600-700 ° C (ma lalo o ka solidus) homogenizes i ka sucd solid solid solud, e hoʻohālikelike ana i ka hoʻoheheʻeʻana ma ka 5-15 ° C.
    ʻo kahi laʻana, ʻO Anneosed C28000 COLITY i kahi aniani o nā 880-900 ° C (vsa. 880-920 ° C no ka mea e like me ka c28000).

5. Nā Kūlana Kūlana (Pehea ka hoʻoholoʻana o nā'āpana meverting)

ʻO ka heluʻana i ka solidus a me nā wai o keʻano keleawe he hana maʻamau.

ʻO keʻano o ke keleawe keleawe
ʻO keʻano o ke keleawe keleawe

Ua hoʻohana pinepineʻia nāʻano maʻamau:

  • ʻO ka carnametyʻokoʻaʻokoʻa (Dsc) / ʻO ka nānāʻana i ka nānāʻana (Dta) - E hāʻawi i nā onset pololei a hoʻopau i nā wela no ka hopena o ka hopena o nā hanana eltingmic, ana i ka wela wela, a he kūpono no ka liʻiliʻi, nā hiʻohiʻona i hoʻomākaukauʻia.
    Hōʻikeʻo DSC Traces i ka hoʻomaka (Nā Sodia Solidus) Ma keʻano he kūlike a me ka hopena nui loa(S) e like me ka wai a me ka wela wela.
  • ʻO ka hoʻomaʻemaʻe-curve (ʻO ka hopuʻana) ʻIkeʻia - ma nā labs i loaʻa, Ua hoʻopaʻaʻia nā moʻolelo TRANUS i ka wā o ka hoʻomehana e hōʻike ana i nā mea hopu hopu (plateuus a iʻole nā ​​loli i loko o ka slope) e pili ana i nā hoʻololiʻana; He pono kēia no ka hōʻoia o ka pono.
  • ʻO ka hopuʻana i ka metalpography - Uaʻaeʻia nā'āpana i kahi mahana i ka mahana o ka mea i loko o ka manawa paʻa-wai a me ka wikiwiki;
    Ke nānā nei i nā hopena o nā microstructures e loaʻa ana i nā mea i hōʻikeʻia ma keʻano he mahana, E hōʻoia i ka nānāʻana i ka nānāʻana.
  • Kuhi Kāleka Kamika (Calphad) - Hiki i nā mea hana kamepiula ke wānana i ka solidus / wai no nā alloys multicomponant a ua nui ka hoʻohanaʻana i nā papa hana.
  • Nā Hana Hana Pono - e ninini ana i nā hana hōʻike hoʻokolohua a nānā i nā hemahema, ʻO nā mea mechanics a me nā microsegregation kōkua kōkua i ka hōʻoiaʻana i nā helu o ka hana ma lalo o nā kūlana hana.

6. ʻO nā palapala noi o kaʻoihana keleawe

ʻO kaʻike pololei o keʻano o ke aniani o ke keleawe he mea koʻikoʻi e hoʻomaʻamaʻa i ka Optimization.

I nā hihia he nui, oia hoi a 10 ° C i hoʻokaʻawaleʻia mai nā mahana kiʻekiʻe hiki ke hōʻemi i ka hāʻawiʻana i nā 20% Ma o nā hemahema e like me nā kuhi hewa, Potiwale, a iʻole zinc collatinization.

ʻO nā hana hana e pili ana i ka hanaʻana i keʻano o ka hoʻohanaʻana i ke kāohiʻana i ka hana hana i ka hana hana.

ʻO keʻano o ke keleawe keleawe
ʻO keʻano o ke keleawe keleawe

Kauhi (Sand cread, Hoolei Make, Hoʻolei kālā)

Koi aku i ke keleawe i ke keleawe i kahi mahana e ninini ana wai + 50-100 ° C, e hōʻoia ana i ka lawaʻana o ka wai e hoʻopiha ai i nā'āpana mold.

Ke kaʻina hana Kakau loa Hoʻohemo melū (° C / ° F) Ka nininiʻana (° C / ° F) Pono ke koi Ke kī nui
Sand cread (Nā brackets automotive) C28000 (Ka hao Muntz) 880-900 / 1,616-1,652 950-980 / 1,742-1,796 Hoʻohaʻahaʻa (Nā'āpana ākea) Ua hōʻemiʻia nā hemahema o ka shrink e ~ 40%
Ikaika loa Hoolei Make (Nā'Āpana Pūnaewele) C36000 (ʻO ke keleawe manuahi manuahi) 870-940 / 1,598-1,724 980-1,020 / 1,796-1,868 High (nā pāʻili <2 mm) Hua >95%, hoʻopiha piha piha
Hoʻolei kālā (Nā mea kani mele) C75200 (Nickel kālā) 1,020-1,070 / 1,868-1,958 1,100-1,150 / 2,012-2,102 Kūpono (ʻO ka geometry paʻakikī) Low poroshity, hoʻomaikaʻi maikaʻi i ka maikaʻi

Welding (Tig, Mohaihala)

Pono ke kumu keleawe e koi ai i ka paleʻana i nā mahana ma luna o ka wai (I mea e pale ai i ka hoʻoheheʻeʻana) ʻOiai e hōʻoia ana i ka wela i ka wela e hoʻopili ai i nāʻili.

  • Tig welding (Nā'āpana keleawe): E hoʻohana i kahi mahana preheat o 200-300 ° C (ma lalo o ka solidus o c26000 keleawe: 1050° C) A me kahi mahana waiʻauʻau o 950-1000 ° C (ma waena o ka paʻa a me ka wai).
    Hoʻohana kēia i kahi "'āpana'āpana" hui "me kaʻole o ka hoʻohemoʻana i ka mea hao waihona.
  • Mohaihala (Nā koho keleawe): E hoʻohana i kahi metala bluzing blazing (E.g., BCUP-2, hoʻomālamalama 645-790 ° C) me kahi wahi e hoʻoheheʻeʻia ma lalo o ka solidus colidus.
    ʻO ka hoʻomehanaʻana i ka 700-750 ° i nā leʻaleʻa filler i ka wā e paʻa ai ke kumu keleawe, Hōʻalo i ka ukiuki hui.

ʻO keʻano hanaʻole: Ma luna o ka lōʻihi o ka cig welding (keka ao >1080° C no C26000 keleawe) ʻO nā kumu "Burn-ma o" (ʻO ka hoʻomālamalamaʻana o ka waihona waihona), koi ana i ka hana a me ka hoʻonuiʻana i nā uku e 50%.

ʻO ka hana wela (Annalile, Ke kaumaha nei ke kaumaha)

Ua kaupalenaʻia nā wela wela wela i nā ma lalo o ka solidus I mea e pale ai i ka hoʻokaʻawaleʻana:

  • Annalile (ʻO nā'āpana keleawe momona): C26000 keleawe he anned i hoʻopauʻia ma 600-650 ° C (vsa. solidus 1050 ° C) e hoʻihoʻi i ka moekolohe (Hoʻonui mai ka engartion mai 10% i 45%) me kaʻole o ka hoʻololiʻana i keʻano o ka uila.
  • Ke kaumaha nei ke kaumaha (Mea koho balota): Wela i ka 250-350 ° C e hōʻemi i nā kaumaha kūlohelohe mai ka machining-i lalo o ka mahana ma lalo o ka solidus, Hōʻalo i nā pōʻino o Microstructural.

7. Ka hoʻoiliʻana & Nā noʻonoʻo palekana o ke keleawe

ʻO Zinc Vaporization a me nā Hazards Fume-Fume

  • Zinc Booli Point e pili ana 907 ° C (≈1,665 ° F). No ka mea he nui nā keleawe maʻamau he nui i nā waiwai e kokoke ana a iʻole ma luna o kēia mahana, Zinc Vaporization aʻo ka hoʻokumuʻana o nā pahu zinc e hiki i ka wā e neʻe ai, ʻO ka uʻi a iʻole ke komoʻana.
    ʻO ka hoʻokomoʻana o Zno Fume hiki ke kumu ʻO ka mea momona momona, ʻO kahi maʻi maʻi flu-like.
  • Hoʻopaʻa nā: ʻO ka hoʻokaʻawaleʻana i ka maʻamau, fume hopu, ʻO ka pale o ke koena, a me ke kāohiʻana o ke aniani i loko o nā hana a me nā hana ulding.

Oxiyan, Dross a me ka mana komo

  • Nā koho balota keleawe (copper a me nā mikike zinc) A DROSS.
    ʻO nā hana a Fluxing a me ka mālamaʻana i nā hana, ʻO Deoxidation Chemistry a me ka nānāʻana i ka Skimming e hōʻemi i ka hoʻopiliʻana o kaxide e hoʻopili ana.
    Hōʻemi nui ka ho'ēmiʻana, hoʻonui i nā hemahema a me nā mea kanu.

Alakaʻi a alakaʻi i nā pilikia regulatory

  • Alakaʻi (Pb) hoʻohanaʻia ma kekahi mau keleawe filena; Loaʻa i nā pae PB liʻiliʻi PB mau mea hoʻoponopono no ka waiʻauʻau a me nā huahana kūʻai.
    Pono e hoʻokeleʻiaʻo alakaʻi alakaʻi alakaʻi i kahi kaʻa kaʻa kaʻa, a me nā huahana i hoʻopau pono e hui i nā hoʻoponopono o nā alakaʻi alakaʻi kūloko.

Desincide a me ka lawelawe lōʻihi

  • Ua lawa kekahi mau keleawe Kaʻanaʻole (ke kohoʻana i ka loaʻaʻana o Zinc) i kekahi mau wai kūpono a me nā wahi.
    ʻO ke kohoʻana o ka dezincification-resistant alloys a iʻole nā ​​hana palekana he mea nui no ka plumbing, Marine a me nā wahi wai wai.

8. Nā kuhi maʻamau maʻamau e pili ana i keʻano o ke keleawe

ʻOiai ke koʻikoʻi o kaʻoihana, Ua kuhi pinepineʻia nāʻano o ke keleawe o ke keleawe. Ma lalo nei he kī nui:

"Ua paʻa ke keleawe" melling point e like me ke keleawe pue. "

Wahahee: ʻO nā lole keleawe maʻemaʻe ma 1083 ° C (paʻaʻia), akā,ʻo ka keleawe-hely-he merting range (paʻa i ka wai).

ʻo kahi laʻana, C36000 keleawe ma waena o 870 ° C a me 940 ° C, ʻaʻole ma keʻano hoʻokahi.

"E hoʻohui hou ana iā Zinc i nā haʻahaʻa haʻahaʻa haʻahaʻa o ke keleawe."

Kahiʻoiaʻiʻo: Zinc ihe i 45% hoʻohaʻahaʻa i ka paeʻana, aka, mamua 45%, zeinc puka i ka brithe γ-phase (Cu₅zn₈, Olinging 860 ° C), a me ka paeʻana o ka menting stbalizes a iʻole ka hoʻonui ikiʻana.

Keleawe-zinc kiʻekiʻe (>50% Zn) ua hoʻohana pinepineʻia ma muli o ka brittleness koʻikoʻi.

"ʻO nā mea nui wale nō keʻano haʻahaʻa o ke keleawe haʻahaʻa haʻahaʻa."

Wahahee: 'Eron (Lia) a me nickel (I) E ho'āla i ka neʻeʻana o ka neʻeʻana ma o ka hoʻokumuʻana i nāʻano kiʻekiʻe kiʻekiʻe. Wale nō "palupalu" imprities (Pb, S) E hoʻohaʻahaʻa i ka palena o ka haunaele.

"Hiki i keʻano o keʻano o ka wela e like me ka lōʻihi e like me ka mea ma luna o ka wai wai."

Wahahee: ʻO ka hōʻeha nuiʻana (wai + >100° C) kumu no ka vinc bolatinization zinc (LOLOHOLOHE >5%) a me ka hana drous, ʻO ka hoʻemiʻana i ka ikaika o ka mīkini.

Kaniʻana (wai + <30° C) alakaʻi i nā mea maikaʻiʻole a me nā mea hoʻopihapiha i hoʻopihaʻia.

9. Hopena

'Ōlelo ʻO keʻano o ke keleawe keleawe ʻaʻole he waiwai paʻa hoʻokahi akā a Nā haʻona ho'ākākaʻia e konaʻano, moloka, a me ka ho'ākākaʻana i ka mōʻaukala.

ʻAʻole like me nā metala maʻemaʻe me nā loli hoʻololiʻana, ʻO ke keleawe-he keleawe-zinc alloy me nā mea hou e like me ke alakaʻi, kū, nickel, a iʻole aluminum-hōʻike a me nā palena paʻa paʻa i kēlāʻanoʻokoʻa.

ʻO kēia mau palena paʻa e pili pono ana i keʻano o ke keleawe i ka wā o Kauhi, Welding, mohaihala, a me nā wela wela, Ke hana nei i ka mana kūpono o ka hoʻoheheʻeʻana i kahi cornestone o ka huiʻoihanaʻoihana.

FaqS

He aha keʻano o ka hoʻomehana o ke keleawe maʻamau i hoʻohanaʻia ma ka plumbing fixture (C26000)?

C26000 (keleawe cretridge) he wela o ka mana o ~ 1050 ° C a me kahi wela wela o ~ 1085 ° C, ka hopena i loko o kahi aniani o ka wai o 35 ° C (1050-1085 ° C).

ʻO kēia'āpana liʻiliʻi e kūpono ai no ke kiʻiʻana i nā piptes i hoʻopaʻaʻia.

Pehea e pili ai i ke alakaʻi alakaʻi i ka neʻeʻana o ke keleawe c36000?

C36000 (ʻO ke keleawe manuahi manuahi) Loaʻa iā 2.5-3.7 wt% alakaʻi.

Kēlā 1 Ua hoʻonuiʻo WT% i ke alakaʻi i ka hoʻohaʻahaʻaʻana i ka wai e ~ 10-15 ° C: a 2.5% ʻO ka helu PB Somple he wai wai o ~ 940 ° C, oiai a 3.7% ʻO Pb Sample kahi wai wai o ~ 925 ° C.

Alakaʻi i nā'āina ākea e hoʻomālamalama (mai 50 ° C a 70 ° C) Ma ka hoʻokumuʻana i nā'āpana haʻahaʻa haʻahaʻa haʻahaʻa.

Hiki iā wau ke koho i ke keleawe me ka hoʻohanaʻana i keʻano like me ke kila?

ʻAʻole. Kukui Kekuhi (E.g., A36) he hoʻoheheʻe wai o 1425-1538 ° C, kiʻekiʻe loa ma mua o ke keleawe.

Keleawe keleawe (E.g., C26000) koi i kahi kiʻekiʻe kiʻekiʻe o ~ 1000 ° C (ma waena o ka paʻa a me ka wai) e pale i ka hoʻohaʻahaʻaʻana i nā mea hao hao-me ka hoʻohanaʻana i nā wela wela e hoʻomehana i ke keleawe.

Pehea wau e ana ai i ka hoʻoheheʻeʻana o ke keleawe ma kahi kūlanaʻoihana?

E hoʻohana i kahi kiʻekiʻe kiʻekiʻe o ka hoʻohaʻahaʻa (pololei ± 5-10 ° C) me kahi papa keleawe 1-5.

E hoʻomoʻa i ka simple ma kahiʻano kiʻi kiʻi, ka monitor mahana me ka thermocouple, a hoʻopaʻa i ka stroidus (ʻO ka hoʻokumu muaʻana) a me ka wai (piha piha) mahana.

ʻO kēia ala ka wikiwiki a kūponoʻole no ka mālamaʻana o Batch.

No ke aha e hoʻohālikelike aiʻo Zinc Voletilization i ka mīkini hoʻohuiʻana o ke keleawe?

Zinc collatinization (ma luna o 907 ° C) ho'ēmi i nā manaʻo zinc o ke keleawe, ka hoʻololiʻana i ka hoʻopiliʻana i ke keleawe.

No ka meaʻo Coppper kahi kiʻekiʻe kiʻekiʻe o ke keleawe ma mua o ke keleawe, ʻO ka papaʻano (solid / wai) hoʻonui.

ʻo kahi laʻana, C36000 keleawe me 3% Ua loaʻa iā Zinc ka nalowale i kahi wai o 960 ° C (vsa. 940° C no ke keleawe hou), e koi ana i ke kiʻekiʻe kiʻekiʻe e mālama ai i ka wai.

Waiho i kahi manaʻo

ʻAʻole e paʻiʻia kāu leka uila. Ua hōʻailonaʻia nā mahina i koiʻia *

E nānā i luna

E kiʻi i ka manaʻo ʻōlelo koke

Eʻoluʻolu e hoʻopiha i kāuʻike a e hoʻokaʻaʻike mākou iāʻoe koke.