1. Hōʻikeʻike
Actoel 600, Ua kohoʻia e like me US N06600 and W. Nr. 2.4816, he nickel-chromium-hao alloy eccessied no ka hana kiʻekiʻe ma wela piha and nā wahi kūlike.
E like me kekahi o nā mea nui e ulu ai i nā hanana incontel, Ua lilo ia i mea waiwai i loko AerERPPACE, Ke kālepaʻana, mana pā'āʻu, a me nāʻoihana moana.
No ka ʻO kahiʻohanaʻo Austenitic, Actoel 600 Hōʻike i ka paleʻana i ka paleʻana i ka oxidation, chordididid -ion kaumaha, a me ka degradation.
Ua hoʻohana nuiʻia ma kahi o nā mea hoʻokūkū hoʻokūkū maʻamau a iʻole nā haʻahaʻa haʻahaʻa haʻahaʻa haʻahaʻa.
2. He aha ka mea e hōʻike ai 600?
Actoel 600 (US N06600) he versetile nickel-chromium-hao alloy Nā mea hana no ka lawelawe ma waena o kahi pālahalaha ākea ākea ʻO nā kūlana cryogenic a hiki i 2000 ° F (1093° C).
Hāʻawi ia i ke kū'ē maikaʻi loa i ka corrosion a me keʻano kiʻekiʻe, e hana ana i kahi mea i makemakeʻia e koi ai i ke koi a me nā wahi kūlohelohe.
Ia ʻO nā manaʻo Nickel kiʻekiʻe Hāʻawi i ke kū'ē kūʻokoʻa chordididid -ion kaumaha, ʻOiai e hāʻawi ana i ka paleʻana i ka paleʻana i kahi ākea ākea o nā hui a me nā hui pū.

'Ōlelo ʻO kaʻikepili chromium Hoʻopili i ke kū'ē ʻO nā Oxidizing, nā mahana ma ke kiʻekiʻe kiʻekiʻe a ma nā pāpā, a kōkua hoʻi i ke kaua sulfur-loaʻa nā hoʻohui.
I nā noi noi kiʻekiʻe, Actoel 600 mālama i ke kūpaʻa hoʻonohonoho a me nā pale Oxidation a me ka scaling a i 2000° F (1093° C).
Hana maikaʻi loa ia i nā kūlana e pili ana Carburization Carburization a iʻole e hōʻike i ʻO nā wahi o keʻano.
Akā naʻe,, Hiki paha ke kānalua luhuahuaia ma lalo o nā kūlana kiʻekiʻe kiʻekiʻe.
Kēia alloy non-magnetic and ʻAʻole hiki ke paʻakikī i ka mālama wela, Akā hiki ke hoʻoikaikaʻia ma o Ke hana anuanu.
Inconel® 600 no laila wellly weldble a kūpono kūpono no ka hoʻoiliʻana i ka hoʻohanaʻana Nā Kūlana Kūʻai Kūʻai.
3. Kemika o ka inconal® 600
Inconel® 600 (US N06600) he hopena paʻa paʻa paʻa nickel-chromium-hao alloy Hoʻolālāʻia no ke kū'ēʻana i ke kū'ēʻana i kahi ākea ākea o nā wahi o nāʻoihana a me nā wela kiʻekiʻe.
Hāʻawi keʻano o keʻano o ke kaila i ke kumu o keʻano o ke kumu no kānaʻano hana mechanical, Ke kū'ē neiʻo Corrosionion, a me ka hana-kiʻekiʻe.
ʻO keʻano koho (% Ma ke kaumaha)
| Mua | Anter (%wt) | Hana / Hana |
| Nickel (I) | 72.0 min | Hāʻawi i ka paleʻana o ka corrossion mua, kumaikalua, a me ke kūpaʻa. |
| Chromium (Cr) | 14.0 - 17.0 | Hoʻonui i ke kū'ēʻana i nāʻoihana a me nāʻano kiʻekiʻe kiʻekiʻe. |
| 'Eron (Lia) | 6.0 - 10.0 | Nā kumukūʻai kumukūʻai a me nā pono hana; hoʻonui i ka ikaika. |
| Mang kāne (Mn) | ≤ 1.0 | Hoʻomaikaʻi hou i ka hana wela a me ka deoxidation i ka wā o ka holoiʻana. |
| keleawe (Cu) | ≤ 0.5 | ʻO nā'ōkuhi corrosiods i loko o kekahi mau hōʻemi hoʻemiʻana. |
| Silikino (A) | ≤ 0.5 | Deoxididhier; e hoʻonui i ka paleʻana o ka oxidation akā mālama i ka haʻahaʻa e pale aku ai i ka brittleness. |
| KālekaʻAʻI (C) | ≤ 0.15 | E hoʻoikaika i ka momi ma waena o ka hoʻonā paʻaʻana i ka paʻakikī paʻakikī akā kaupalenaʻia e hōʻemi i ka embrittlement. |
| Sulfur (S) | ≤ 0.015 | Poino; kāohiʻia e hoʻonui i ka hana wela a me ka weldtability. |
4. Nā mea waiwai nui o ka inconal 600
Inconel® 600 (US N06600) ua hanaʻia mechanical ingority and ke kū'ē kū'ē Ma lalo o ke koiʻana i nā kūlana a me nā kūlana kūpono.

Nā Pīkuhi Propertinies
| Waiwai | Waiwai maʻamau (I ka lumi) |
| Ikaika ikaika | 655 Mpa (95,000 Psi) |
| Ka ikaika (0.2% Kahiki) | 310 Mpa (45,000 Psi) |
| Ewangantion (% i 50 mm) | ≥ 30% |
| Hālulu (Rockwell b) | 85-90 |
| Modulus olasticity | ~ 207 GPA (30 x 10³ ksi) |
| Hopena paʻakikī (Chary v-notch, 20° C) | > 100 J (MAKAINA WAU) |
Nānā: ʻO nā waiwai kūpono e like me keʻano o ka palapala huahana, Kohano, a me nā wela wela. Hoʻonui ka hana anuanu i ka ikaikaʻoiai e hōʻemi ana i ka lōʻihi.
ʻO nā waiwai pale o Corrosionion
Actoel 600 kū i kahi ākea ākea o nā wahi o ke kuʻekuʻe ma muli o kona kiʻekiʻe nickel and Chromium anter:
- Chordid -on scc pale: Aneane immune, ʻOiai i loko o nā hopena wela a me nā hopena choroide.
- ʻO ka pale oxidation: E kūpono a hiki i 1093 ° C (2000° F) I ka lewa a me nā mea hoʻonaninani.
- ʻO ka paleʻana o ka laweʻana: Mālama pono i ka intgrity ma nā anianiʻoihanaʻoihana waiwai.
- ACID a me SNESSNING SONSISTANCE: Paʻa i nā wahi nui a me nā wahi alkaline (E.g., Nitric, lupulakai, sodium hydroxide).
- Manea Hana: Ke kū'ē maikaʻi i ke kai a me brine, ʻOiaiʻaʻole ia he mau mea hana crevice corrosio ma lalo o nā kūlana stagnant.
5. ʻO nā waiwai pilikino o ka Inconel® Alloy 600
Inconoel® alloy 600 (US N06600) hōʻike i kahiʻano o nā mea pilikino e hāʻawi ai i kāna hana kūʻokoʻa i nā wahi nui loa.
| Waiwai | Waiwai maʻamau |
| Huakai | 8.47 g / cm³ (0.306 lb / in³) |
| Hoʻomālamalama Nā haʻona | 1354 - 1413 ° C (2470 - 2575 ° F) |
| Ka HōʻaʻO Kokua | 14.8 W / m · c · i ka 100 ° C |
| ʻO ka mana wela (Kepana) | 0.444 J / g · g na o 25 ° C |
| ʻO keʻano o ka uila | 103.4 μω · HUA MA 20 ° C |
| Ka maikaʻi o ka hoʻonuiʻana i ka | 13.3 μM / m · m · ° C (20-1000 ° C) |
| Modulus olasticity | 207 GPA (30 P× 10³ KSI) |
| ʻO Magnetic Permeibility (m) | ~ 1.0006 (non-magnetic) |
| ʻO ka laulā o Poisson | 0.30 |
| Leo anehuki (longitidinal) | ~ 5,050 m / s (I ka paʻa) |
6. ʻO ka hana kiʻekiʻe kiʻekiʻe o nā hanana o Inconoel® alloy 600
- ʻO ka pale oxidation:
E nānā i ka oxidation a me ke kaʻeʻana i nā mahana a hiki i 2000 ° F (1093° C), ka mālamaʻana i nā mea kūpono a me nā mea hana pono. - ʻO ka paleʻana o ka laweʻana:
Hana maikaʻi ma nā wahi kaʻa kaʻa, Ke hoʻopau nei i ka carbon e pili ana a mālama pono i ka paʻaʻana. - Kālea kakahiaka:
Hāʻawi i ke kū'ēʻana i ke kū'ēʻana i ka suldidation ma nā wela kiʻekiʻe akā hiki ke hōʻoleʻia i loko o nā pae kiʻekiʻe o Sulfide. - Paʻa wela:
Mālama i ka ikaika mechanical a paʻakikī i ka wā iʻikeʻia i kaʻike lōʻihi i nā kiʻekiʻe kiʻekiʻe a me keʻano. - Incrutural integrity:
Ua ulu nui ka uluʻana o ka palaoa, pale aku i ka brittleness a iʻole ka deformation i ka lawelawe. - PAHUI:
Hiki i ka hana ke hoʻopau i nāʻenehana e hoʻopili ana i ka wela wela me nā mea e kū pono ai (E.g., NA LOUGU ALOHA), e pono ai i nā mea hou aku no ia mau kūlana.
7. Huahuai & Machineability o Inconel® Alloy 600
Inconoel® alloy 600 (US N06600) ua hanaʻia ʻO ke kūpaʻa kiʻekiʻe a me ke kūlana, aka, ua haawi aku ia hana maikaʻi loa ma waena o nāʻano hana maʻamau maʻamau.
Hiki iā ia hana wela, anu-hana, welded, a me ka machini Ke hoʻohana nei i ka hana maʻamau i hoʻoponoponoʻia e pili ana i kona ikaika, hana hana-paʻakikī, a me ke kūpaʻa metallirgical.

Kauhi
ʻOiaiʻaʻole like me ka mea maʻamau 718, Actoel 600 hiki Kālā-lawena-mālama i loko o nāʻano paʻakikī (E.g., nā kino valve) Me nā mea paʻa paʻa (± 0.1 mm).
Koi aku i ke kāʻeiʻana i ka ho'ōlaʻana e pale ai i ka paleʻana o ka crabide, hiki ke hōʻemi i ka ductility.
Ka hana wela
Actoel 600 he ductile maikaʻi loa i ka wā i hanaʻia ai ma ke kiʻekiʻe kiʻekiʻe, e hana maikaʻi ana i nā hana wela wela e like me ke kalaʻana, hānehi, a lele.
- Ua hōʻikeʻia ka wela wela wela:
870-1230 ° C (1600-2250 ° F) - Huhū kaumaha (Kākau, Hānehi):
1040-1230 ° C (1900-2250 ° F) - Mālamalama (E hoʻopau i nā hala, misping shaping):
E like me 870° C (1600° F) - Hōʻalo i nā hana hana:
650-870 ° C (1200-1600 ° F) - Ma muli o ka hoʻemiʻana i ka lōʻihi a me ka pilikia o ka microcraccking.
No nā hopena maikaʻi loa, E hele pū me ka hana wela e like me ka hoʻohuiʻana a me ka rapid qualching e hoʻihoʻi i ka paleʻana i ka paleʻana a hoʻomaha i nā kaumaha kūloko.
Keʻano anuanu
Actoel 600 hiki anu-hana Ke hoʻohana nei i nā hana e like me nā mea no nā kinikini paʻakikī a me nā mea haʻahaʻa haʻahaʻa.
Hōʻike ia ʻoi aku ka nui o ka hanaʻana ma mua o ke kilokilo, ʻOiaiʻo ia ke kala houʻana ma mua o keʻano 304 kila kohu ʻole.
- Hana Hoʻolālā: Kulou ana, hukiʻulu, noho ', 'ahuʻu
- Mau olelo:
-
- Pono paha ke kikowaena waena no ka paʻakikī a iʻole ka hohonu hohonu.
- ʻO ka lubrication a me nā mea hana e kōkua ai i ke kōkuaʻana i ka mālama ponoʻana i ka dimensional.
Hoʻonui ka hana anuanu i ka ikaika a me ka paʻakikī akā hiki ke hōʻemi i ka ductility-anneataling-anenenging.
Welding
Inconoel® alloy 600 hōʻike maikaʻi loa ma waena o nāʻano hana kiʻekiʻe a pau, a ua nui ka hoʻohanaʻana i ka hoʻoikaikaʻana i nā noi a me nā noi a me nā noi e pono ai e hoʻomaʻemaʻe, Nā 'ōlelo-manuahi.
- Nā kaʻina hana e pili ana:
-
- Gtaw (Tig)
- Kāmaʻa kikomua (Me / Mag)
- Smaw (Lāʻau / mma)
- Plasma arc
- Hoʻonohonohoʻia nā metala:
-
- Ernicr-3 (no tig a me aʻu)
- Enicrfe-3 (No ka pua pua)
- ʻO ka hana wela wela (Pwht): ʻAʻole pono e koiʻia, ʻOiai e hoʻopiliʻia ke kaumaha-relief no nā'ōnaehana koʻikoʻi.
Ke hoʻopau nei i ka helu: Ma hope o ka welding, brush me a ʻO nā mea kila kila kila Hoʻopau i nā'āpana wela, Ke waiho nei i kahi papa maʻemaʻe me kaʻole e pono hou no kaʻohiʻana.
Machimen
Hoʻopiliʻia ka hana ma keʻano o Inconoel 600 i nā alloys kiʻekiʻe-Nickel. Oiai ʻOi aku ka maikaʻi o ka machninability ma mua o 304 meaʻole, he mau i ka haʻahaʻa i nā helu manuahi manuahi 303.
Nā hiʻohiʻona makika:
- ʻO ke kūlana maikaʻi maikaʻi maikaʻi loa: Anned
- Hana-paʻakikī paʻakikī: Pono nā mea kiʻekiʻe - nā mea pāʻani eʻokiʻia ma lalo o ka papa paʻakikī
- ʻOkiʻoki i nā wikiwiki: Hoʻohaʻahaʻa, me ʻO ka komoʻana e komo ai
- Mea hana: Ua hāʻawiʻia nā mea hoʻonaninani a iʻole cramic
- 'Ōpala: Ikaika nui, Pono ka wai e pili ana i ka wai
| Machining factor | Hana maikaʻi loa |
| Hualoaʻa | ʻO ke kiʻekiʻe kiʻekiʻe (Hōʻalo i kaʻohiʻana) |
| Hohonu o kaʻokiʻoki | Lawa e hoʻonui ai i ka papa paʻakikī |
| Hoao | ʻO nā kāpili a iʻole nā mea i hoʻopiliʻia; Hōʻalo i nā mea hana hana |
| Kūkaha | Hoʻohanaʻia ka hoʻohanaʻana i nā mīkini rigid a me nā hana hana hana |
| Lubrication | ʻO ke kāhiko o ka wai e hōʻemi ai i ka kūkulu hale |
8. Noi o inconel 600
ʻO ka huiʻana o Inconoel® alloy 600 ka ikaika kiʻekiʻe, Ke kū'ē neiʻo Corrosionion, a me nā hiʻohiʻona maikaʻi hana ia i nā mea i koiʻia i nā koina o nāʻoihanaʻoihana.

| ʻOihana Kahuna | Nā'āpana maʻamau | Loaʻa nā kiʻi nui |
| Pono & Aila | Nā Vilves, ʻO nā mea hana i lalo, flanges | Ke kū'ē neiʻo Corrosionion, ikaika ikaika |
| Mana pā'āʻu | Nā mea hana Steam, superhoeters, Nā huakaʻi kuʻuna | ʻO ka paleʻana o ka oxidation kiʻekiʻe, kūlohelohe |
| Ke kālepaʻana | Nā mea hana wela, nā ipu koʻikoʻi | Ke kū'ēʻana i nā lāʻau lapaʻau a me nā mea hoʻonaninani |
| Aerospace | Nā keʻena hui, Aloha, Nā mea paʻa | ʻO ka ikaika kiʻekiʻe, cyclic thermal pale |
| Marine | Pumps, Nā Vilves, Nā Pūnaewele Subseea | Chordide corrosiotion resistion, ka wai kai kai |
| Cessogen & Meaʻai | Nā Kūkahu Kūʻai, ʻO ka hoʻoiliʻana i nā lako | Paʻakikī, Ke kū'ē neiʻo Corrosionion |
9. Loaʻa a me nā palena
Loaʻa i nā hanana o Inconel 600
- ʻO ka hana kiʻekiʻe kiʻekiʻe:
Mālama i ka ikaika mechanical a me ka oxidation resistance a hiki i ka 1,095 ° C, Me ka paleʻana o ka creep creep a me ka paʻa paʻa. - Ke kū'ē neiʻo Corrosion Corrossion:
Ka paleʻana i kahi ākea ākea o nā wahi o nā wahi e pili ana i ke kai, ʻO nā maʻi maʻi, a me ke kaumaha o ke kaumaha o ke kaumaha. - ʻO ka lole maikaʻi:
Maʻalahi maʻalahi a me ka hanaʻana me ka hoʻohanaʻana i nāʻano maʻamau; matchinable me nā mea kūpono kūpono i ka hana paʻakikī. - ʻO nā meaʻole-magnetic a me ka radiation pale:
ʻO kānaʻano Austetitic e hōʻoia i keʻano hana a me ka hana maikaʻi a me ka hana maikaʻi ma nā wahi e pili ana i nāʻenehana nuklea i hōʻikeʻia i ka radiation.
Nā palena o ka inconal 600
- Palena palenaʻole i nā maʻi ikaika:
Hoʻoweliweliʻia eʻike i nā maʻi hydrochloiric a hui pūʻia, Ke hoʻohana nei i ka hoʻohanaʻana i nā wahi e pono ai. - Hoʻopau ka ikaika i nā kiʻekiʻe kiʻekiʻe:
Nā manaʻo noʻonoʻoʻo Mechanical i hōʻikeʻia ma luna o 815 ° C, ʻO ka hoʻohanaʻana i ka hoʻohanaʻana i nā noi e ultra-kiʻekiʻe-kiʻekiʻe e like me Turbine Blades. - Uku kiʻekiʻe:
ʻOi aku ka nui ma mua o nā mea iʻoi aku ma mua o nā mea hoʻokūkū maʻamau ma nā'ōlelo a me nā kumukūʻai. - ʻO ka nānāʻana i ka wela wela:
Koi pono i ka hoʻokaʻawaleʻana e pale ai i ka mea i hiki ke hōʻemi i ke kū'ēʻana.
10. Hoʻohālikelike me nā alloys'ē aʻe
| Waiwai / Alloy | Actoel 600 | Actoel 625 | Kila kohu ʻole 316 | Wikiwiki c-276 |
| Ka Hoʻolālā | ni-c c-f-fe (Koho Koho. 72% I) | In-cr-i (ʻoi aku ka nui o nāʻike) | Makemake-c-in-i | I-i-cr-fe |
| ʻO kaʻoihana lawelawe kiʻekiʻe | A hiki i 1,095 ° C (2,000° F) | A hiki i 982 ° C (1,800° F) | A puni 870 ° C (1,600° F) | Na i 1,093 ° C (2,000° F) |
| Ke kū'ē neiʻo Corrosionion | Maikaʻi loa i nā maʻi maʻi & Ke wai wai; kaupalenaʻia i nā maʻi ikaika | ʻOi aku ma ka oxidizing & hoʻemi i nā wahi; ʻO ka pitting maikaʻi loa & crevice resistance | ʻO ke kū'ēʻana o ka'ōpū; ilihune i loko o nā hui chlordide | ʻO ka paleʻana i ka paleʻana i ka oxidizing / hoʻemi i nā maʻi a me ka chrlode |
| Ka ikaika ikaika | ʻO ka ikaika kiʻekiʻe-kiʻekiʻe | ʻOi aku ka ikaika kiʻekiʻe ma muli o ka hoʻoikaika paʻaʻana | Ikaika | Ikaika ikaika a me ka paʻakikī |
| Huhu | Maikaʻi maikaʻi a me ka mancinability | Mea maikaʻi; ʻoi aku ka paʻakikī paʻakikī | Maikaʻi loa a me ka mancinability | Paʻakikī i ka mīkini a me ka weld |
| Kālā | ʻO ke kiʻekiʻe kiʻekiʻe | ʻOi aku ka kiʻekiʻe ma mua o ka inconal 600 | Uku haʻahaʻa | Kumukūʻai kiʻekiʻe |
| Nā noi maʻamau | Nā mea hana wela, Nā Vilves, nā mea hana nuklea | Aerospace, Ke kālepaʻana, Marine | ʻO ka ho'ōlaʻana i ka meaʻai, olakino, ʻOihana Makahiki | Nā mea hana loiloi, ke kāohiʻana, ʻO nā wahi kūlike loa |
11. Nā kūlana & Nā Palapala Hoʻohui
| Kū-starder | ʻO ka weheweheʻana |
| Kā mākou | N06600 |
| W. Nr. | 2.4816 |
| Hosm | Na B166 (Kāla Rulu, Bar), Na B167 (Huhū), B168 (She wallpaper) |
| Meme | Sb166, Sb167, Sb168 |
| Amp | 5540 (She wallpaper), 5665 (PANA / Kakau) |
12. Hopena
Actoel 600 E hoʻomau i kahi pou o kaʻenehana hana kiʻekiʻe, Hāʻawi i kahiʻano kūʻokoʻa o keʻano kiʻekiʻe, Ke kū'ē neiʻo Corrosionion, a me ka moekolohe.
Kona hiki ke ulu i nā wahi o nā mea hana nui loa-mai nā mea hana nukle ma nā wahi hohonu o ka wai hohonu.
ʻOiaiʻo Newer Alloys Excel i nā noi Niche, ʻO ka kaulike o Inconel 600 o nā waiwai a hōʻoia i ka hoʻopaʻa inoaʻana i ka hoʻopaʻaʻana i ka hoʻomauʻana i ka pilina koʻikoʻi.
E like me nā meaʻenehana e koi ai, kona kuleana e like me ka hilinaʻi, E hoʻomau mau ka manaʻo nui.
Nāʻatikala e pili ana: https://www.specialmetals.com/documents/technical-bulletins/inconel/inconel-alloy-600.pdf
FaqS
He aha ka nokel alokel 600?
Nickel alloy 600 (Inconel® 600) he hana kiʻekiʻe, ʻO nā mea i hoʻohuihuiʻia non-magnetic, Chromium, a hao hao.
Heʻenehana ia no ka hoʻohanaʻana i loko ʻO ke kiʻekiʻe nui a me nā wahi hoʻoponopono, nui loa ma ka aerospace, Ke kālepaʻana, a me nāʻoihana moana.
He aha ka mahana o ka lawelawe kiʻekiʻe loa no ka inconal 600?
Actoel 600 hiki ke hana mau i nā mahana i nā mahana a hiki i ka 1,095 ° C ma oxidizing inika, Me ka hōʻike pōkole pōkole i 1,200 ° C hiki.
Inconal 600 magnetic?
ʻAʻole, ʻO kāna microstruc microstruc micstructure e hanaʻole ai, He waiwai koʻikoʻi no nā mea i loaʻa i nā mea i hoʻopaʻaʻia i ka mea i hōʻikeʻia (Mri) nā lako hana a iʻole nā electromagnetic.
Hiki i ka pilikia 600 e hoʻohanaʻia i nā noi o ke kai?
ʻAe, ʻO kāna helu corrosio ma ke kai kai <0.01 MM / makahiki, Ke kūpono nei ia i nā mea hana marine hardware e like me nā pumps, Nā Vilves, a me nā mea kālepa wela.
Pehea ka hanaʻana 600 Hoʻohālikelike iā Inconel 718?
Actoel 600 Hāʻawi i nā pale o ka oxidation maikaʻi aʻoi aku ka nui o ke kumukūʻai, oiai 718 Hāʻawi i ka ikaika kiʻekiʻe ma nā wela kiʻekiʻe (E piʻi i 980 ° C) Ma muli o kāna hana pio-paʻakikī paʻakikī.
He aha ke kumu o ka embrittlement ma inconal 600?
ʻO nā pale i nā palena i nā palena palaoa i ka wā o ka mālama ponoʻana i ka wela (E.g., lohi mālie mai 600-800 ° C) hiki ke kumu i ka make. Ua paleʻia kēia ma ka hoʻonāukiukiʻana i ka 1,095 ° C i ukaliʻia e REPID.