A383 alumini alloy e kū ana ma keʻano he mea kūikawā i loko o ke kumukūʻai kiʻekiʻe, E hoʻokaʻawale e hāʻawi i ka ikaika kūpono, Hoʻopiliʻia ke kū'ēʻana, a me nā hale kūʻai kiʻekiʻe.
Ua hoʻomohalaʻia kēia alloy ma kahiʻano'ē aʻe i A380, hāʻawi i kahi hoʻomaikaʻi nui i ka paleʻana i ka paleʻana a me kaʻoi aku ka maikaʻi o ke kaheʻana.
Ma kēiaʻatikala, Hāʻawi mākou i kahi paʻa, ka nānāʻana i ka nānāʻana o A383, keʻimi nei i kānaʻano, Nā Pūnaewele Pūnaewele, Ke kaʻina hanaʻana, nā noiʻenehana, Loaʻa, mea paʻakikī, a me nā manaʻo.
1. Hōʻikeʻike
Ua pāʻaniʻo A383 alumini alloy i kahi hana koʻikoʻi ma keʻano he nui, hana no ka hanaʻana i nā mea hoʻohālikelike, Nā'āpana'āpana.
Nā mea hana i ka kaʻa, mea uila, a me nā mea hanaʻoihanaʻoihana e hoʻohuli i ka huliʻana i A383
Ke koi nei lākou i kahi mea i hāʻawiʻoleʻia e hāʻawi wale i ka hana mechanical a me nā liʻiliʻi a me nā mea liʻiliʻi.
I nā makahiki i hala iho nei, ʻO ka neʻeʻana o ka aluluni e make ai i nā mea e hoʻopiliʻia aiʻo A383 i ka mua, ka hoʻokeleʻana e nā koi o ka mākeke a me nā holomua ma kaʻenehana hana hana.
Ua wānana nā mea kūʻai aku hou i nā koina o ka honua no ka hoʻomaʻamaʻa kiʻekiʻe
e ulu nui i kahi helu ulu ulu (Cagr) o A puni 5.2% ma luna o nā makahiki e hiki mai ana, ʻO Underscoring A383.
2. He aha ka alow03?
A383 no kaʻohana o ke kiʻekiʻe o keʻano o ke kaomi kiʻekiʻe-sticonum-silicon alloys.
Ua hoʻolālāʻiaʻo ia ma keʻano he ala'ē aʻe i ka A380, me nā hoʻomaikaʻiʻana i ke kū'ēʻana i keʻano wela a me ka hoʻonuiʻiaʻana.
Hiki i kēia hui hoʻohālikelike i ka leka uila A383 e hoʻopiha i nā geomex, ʻO ka hana kūpono no ka hanaʻana i ke kiʻekiʻe kiʻekiʻe, nā'āpana'āpana i hoʻopaʻaʻia ma ka hana kiʻekiʻe.

3. Kalepa me nā micsopy a me nā micsostructure
A383 alluinum alloy e hoʻomaʻamaʻaʻia e hoʻokō i nā koi o ke kumu kiʻekiʻe e make ai ma ka hāʻawiʻana i kahiʻano kūpono kūpono e hoʻonui ai i keʻano o keʻano.
ʻO kānaʻano hana a me ka microstructure e pāʻani i kahi hana pivotal i ka hōʻoiaʻana i ka mālama maikaʻi, hoʻemiʻia nā hemahema, a hoʻomaikaʻi i ka hana i ka paʻakikī, Nā'āpana'āpana.
Kinohi
Aia ma lalo nei he papaʻaina e hōʻuluʻulu i nā mea nui i nā mea nui ma A383 aluminum Alloy, ko lākou hui maʻamau maʻamau, a me kā lākou hana mua:
| Mua | Ka Hoʻolālā (%) | Hana & Hopena |
|---|---|---|
| Aluminum (AL) | Kaulike | ʻO ka mea hao waihona e hāʻawi i keʻano kūpono. |
| Silikino (A) | 10.0 - 11.0 | Hoʻomaikaʻi i ka wai, E kāʻei i ke kū'ē, a hoʻemi i ka hoʻonuiʻana i ka hana. |
| keleawe (Cu) | 2.0 - 3.0 | Hoʻonui i ka ikaika a me ka paʻakikī akā hiki ke hōʻemi iki i ke kū'ēʻana. |
| Magnesum (Mg) | 0.1 - 0.3 | Hoʻonui i ka ikaika a hoʻomaikaʻi i ke kū'ē kū'ē. |
| 'Eron (Lia) | ≤ 1.3 | Kōkua i ke kāohiʻana a hoʻomaikaʻi i nā waiwai, Akā hiki i nā mea nui ke hōʻemi i ka ductility. |
| Zinc (Zn) | ≤ 3.0 | Hoʻomaikaʻi hou i ka hana holoʻokoʻa holoʻokoʻa a me ka ikaika. |
| Mang kāne (Mn) | ≤ 0.5 | Hoʻonui i ke kū'ēʻana i ka deformation a me kaʻokiʻana. |
| Nickel (I) | ≤ 0.3 | Hoʻonui i ka ikaika ma nā kiʻekiʻe kiʻekiʻe. |
| Kū (Sno) | ≤ 0.15 | ʻO nā liʻiliʻi liʻiliʻi i loko o nā noi kiʻekiʻe. |
| Nā mea'ē aʻe | ≤ 0.5 (Nui) | Nā meaʻona liʻiliʻi e kōkua ai i nā waiwai maikaʻi. |
Nā hiʻohiʻona microstrucher
ʻO ka Microstructure o A383 alumini alloy e pāʻani ana i kahi hana koʻikoʻi ma kāna hana, i loko o nā noi noi e make ai. Aia ia i nā hiʻohiʻona koʻikoʻi:
- ʻO nā hana alumini-waiwai nui a me nā mea hana silika silika: ʻO nā hana alloy alllonum-waiwai waiwai waiwai me ka nui o nā silini silika silitic.
Hoʻokomoʻia kēiaʻano hoʻonohonoho i ke kū'ēʻana a hōʻemi i nā hemahema. - ʻO keʻano maikaʻi maikaʻi: Hōʻikeʻo A383.
ʻO ka nui o ka nui liʻiliʻi i hāʻawiʻia i ka nui o ka paʻakikī a me ke kūpaʻa kiʻekiʻe. - ʻO ka paleʻana i ke kū'ēʻana: ʻO ka mea i hoʻonuiʻia i kaʻike Silikino ma A383 e hōʻemi i ka pilikia o ka huki wela i hoʻohālikelikeʻia i nā alloys'ē aʻe, e hana ana i kahi kūpono kūpono no ke komoʻana, nā hoʻolālā maikaʻiʻole.
- Ke kāohi neiʻo Poosity: Kūpono kūpono a me ka mālamaʻana i ka hopena o ka ho'ōlaʻana i kahi microsructure hou aʻe, ʻO ka hōʻemiʻana i nā pilikia poosity i nā mea maʻamau ma keʻano kiʻekiʻe.
4. ʻO nā waiwai pilikino a me nā mīkini
Hāʻawiʻo A383 alumini alloy i kahi hui kaulike maikaʻi o ka ikaika mechanical, kumaikalua, hana thermal, ka mea e kūpono ai i nā mea e koi ai i nā noi.
ʻO kāna hui kūʻokoʻa o nā waiwai e hiki ai i nā mea hana e hana i ka paʻakikī,
nā mea i kohoʻia e mālama i keʻano o ka hoʻonohonohoʻana ma lalo o ke kaumaha ma lalo o ke kaumahaʻana i keʻano maikaʻi a me ka dimensional maikaʻi loa.
Ikaika a me ka paʻakikī
- Ikaika ikaika:
Ua loaʻa i A383 E loaʻa i nā ikaika o TRSILE TERSILE ma ka laulā o 310-322 mpa, Ke hōʻoia nei e hoʻolei i nā'āpana i nā mea nui.
Kākoʻo kēia ikaika i nā noi noi e noi ana i ka hana i ka hana ma lalo o ke kaumaha mechanical. - Ka ikaika:
Me ka nui o ka ikaika a puni 150-160 mpa, A383 E pale aku i ka nānāʻana i ka wā o ka lawelawe.
ʻOiai liʻiliʻi ma lalo o kekahi mau hoʻokūkū hoʻokūkū e like me A380, Hāʻawi kēiaʻano hiʻohiʻona i ke kū'ēʻoi aku ka maikaʻi o ka paleʻana i ka wela i ka wā o ke kaʻina kūʻai. - Hālulu:
Hāʻawiʻo A383 i kahi kūlana paʻakikī e hāʻawi ai i nā mea e pono ai e pale i ka paleʻana no nā noi he nui.
Ke kākoʻo nei kona paʻakikī i ka hana o nā mea eʻike ai i ka hoʻopili maʻamau, e hana ana i kahi koho maikaʻi loa no nā'āpana e pono ai e mālama i kahi kūpono, ka lōʻihi lōʻihi.

Kupono a me ka ellingation
- Elongation a me ka formability:
A383 mau hōʻike i hoʻonuiʻia i ka ductity i hoʻohālikelikeʻia i kekahi mau mea e make ai.
Kona hele, ka maʻamau a puni 3-4%, E hōʻoia i ka mea e mālama ai i kahi pae kiʻekiʻe o ka wikiwiki, ka hōʻemiʻana i ka pilikia o ka brittle frittle i ka wā lawelawe a me ka lawelawe.
Hāʻawi kēia no ka hana no ka hanaʻana no ka hanaʻana i nā geometrite geometries me kahi haʻahaʻa haʻahaʻa o nā hemahema e like me ka huki wela.
Nā'lelo Thermal
- Ka HōʻaʻO Kokua:
Me nā mea waiwai a ka thermal a puni 90-100 w / m · k, A383 kūpono i ka wela.
Ua hōʻoia kēia waiwai i ka pōmaikaʻi i nā noi e like me nā mea uila a me nā mea wela wela, kahi e pono ai ka hoʻokele waiwai maikaʻi. - Paʻa wela:
E mālamaʻo A383,
Ke hōʻoia nei e hana i nā mea i hana pono i nā wahi kiʻekiʻe, e like me nā'āpanaʻenehana a iʻole nā mea hana mana mana.
Ke kū'ē neiʻo Corrosionion
- Hoʻopiliʻia ke kū'ēʻana:
ʻO ka huiʻana o ka alloy, ʻO kā kāna mea kūʻai keleawe i hoʻopaʻaʻia, hāʻawi i ke kū'ē i ka paleʻana i ka corrosion i hoʻohālikelikeʻia i nā alloys like me A380.
A383 hana maikaʻi loa i loko moios, ʻO nā mea waiwai waiwai-waiwai, Ke kūpono nei i kūpono no nā noi automotive a me nā mea hana ma kahi eʻikeʻia ai nā mea i hōʻehaʻia.
5. Ka hoʻoiliʻana a me nā hana hana hoʻolālā
ʻO A383 allminum alloy a me nā microstructure e noi ana i ka hanaʻana i ka hoʻoiliʻana a me nā hana hana hana e mālama ai i kāna waiwai maikaʻi.
Hana nā mea hana i nāʻanoʻano likeʻole-mai ka makeʻana i ka makeʻana e holomua i ka machivanced.
Ma lalo, Eʻimi mākou i kēia mauʻenehana a kūkā pehea e koho ai lākou i ka hanaʻana i ka hana aʻo ka mālamaʻana i ka maikaʻi a me ka hana.
Make i ka mālama ponoʻana
A383 EXTELY ma keʻano kiʻekiʻe make buring Ma muli o kāna mea maikaʻi loa a me ka hoʻoponopono wikiwikiʻana. ʻO nā mea hana hana e hoʻopiʻi i kekahi mau kī nui e hōʻoia i ka maikaʻi:
- Mold mahana: Ka mālamaʻana i kahi wela wela (ma waena o 200-250 ° C) Hoʻopau i nā hoʻopiha piha piha a hōʻemi i ka hopena o nā hemahema.
- ʻO ka wikiwiki a me ke kaomi: E hoʻoponopono ana i nā wikiwiki injection (pinepine ma ka pae o 50-100 m / s) a me nā koi (a i 30,000 Psi) mimilizes shrinkis a me nā poosity aʻo ka hōʻoiaʻana i kahi lole, hoʻopiha piha.
- ʻO nā uku hoʻomehana: E kōkua nā kumukūʻai hoʻonaninani e kōkua i ka hōʻemiʻana i nā kaumaha ola a hōʻemi i ka huki wela wela. Hiki i nā mea hoʻonaninani hoʻomaʻemaʻe maikaʻi e hoʻomaikaʻi i ka hāʻawiʻana e like me ka nui o 10-15%.

Matching a me ka hanaʻana
Ponoʻo A383 a A383 i ka pololei o ka mea i kohoʻia aʻokiʻoki i nā'āpana:
- ʻOkiʻana i nā hana hana: E hoʻohana i nā mea hana kaʻa a iʻole nā mea hana i keʻano wela nui e pale aku ai i nā mea e hoʻopili ai i nā mea hana rapid i hanaʻia e ka ikaika kiʻekiʻe a me ka ikaika ikaika.
- ʻO nā wikiwikiʻokiʻoki: Mālama i nā wikiwiki e hōʻoki ana i nā wikiwiki (a puni 20-40 m / min) I mea e pale ai, a e hoʻohana i nā uku momona e hōʻemi i ka kaumaha ma ke kihiʻokiʻoki.
- 'Ōnaehana Papa: He mea nui nā'ōnaehana kiʻekiʻe-kiʻekiʻe. Kōkua lākou i ka hōʻoleʻana i ka wela wela, mālama i ke ola hana, A e hōʻoia i kahiʻoki maʻemaʻe.
- Post-ho'ōla: Ma hope o ka Machining, Hiki i nā'āpana i nā mea i hanaʻia e like me ke anading a iʻole ka uhiʻana a iʻole ka hanaʻana i nā pale e hoʻonui hou aku ai a hoʻomaikaʻi hou.
Ke kōkua nei kēia mau wāwae i ke kaumaha o nā mea kaumaha i ka wā o ka machining.

ʻO ka hana wela a me ka hoʻopauʻana
ʻOiaiʻo A383ʻaʻole i mālama pinepineʻia, Hiki i kekahi mau noi ke pōmaikaʻi mai nā kaʻina hana i kāohiʻia e hoʻonui ai i nā waiwai kiko'ī.
- Hoʻoholo hōʻoluʻolu: Ka hōʻehaʻana i ka alloy a 1100-1200 ° C, ukali e rapid quanching, ʻO nā paleʻole i nā mea i hikiʻole ke hoʻonuiʻia a hoʻonui i ka ductility.
- Kaumaha e hōʻoluʻolu ai: Ke hana nei i ka hoʻomahaʻana i ke kaumaha ma ka 800-900 ° C e hōʻemi i nā kaumaha o ke koena a me ke kalaʻana, e hōʻoia ana i ka paʻaʻana i nā'āpana ma lalo o nā ukana cyclic.
- Nā hana mālama: Ke kāohi nei i nā kaʻina hana nui e hoʻopaʻa ana i keʻano grain a hoʻonui i ka kaulike ma waena o ka ikaika a me ka paʻakikī.
- PAHUI:
-
- ʻAʻole e pane maikaʻiʻo A383 i nā lāʻau wela e like me T6 e huhū ana, he mea maʻamau no nā alloys'ē aʻe.
Ke hoʻopauʻana:
- Uilaiauliwi: Hana i kahi kūpono, ʻO keʻano o keʻano o ka hanaʻana i ke kū'ēʻana.
- Hoʻolauna: Hoʻoikaika i ka hana kūlohelohe, ka paleʻana i ka alloy i nā wahi hoʻohālikelike.
- Pio ke pale: Ke noi nei i ka ptfe, hana, a iʻole e hoʻonui i nā lole pvd i ke ola o nā'āpana o nā'āpana i nā kūlana kūpono a iʻole nā kūlana kiʻekiʻe.
- ʻO ka pauka: Hoʻolako i kahi paʻa, Hoʻokipaʻia i ka wā e hoʻomaikaʻi ana i ke kū'ēʻana i nā mea kūlohelohe.
ʻO ka Welding a me ka hui pūʻana
ʻAʻole i'ōleloʻiaʻo A383 no ka ulia no ka mea i hiki ai i kona kānalua e hoʻopili ai a me ka parosity.
Nā Kūlana Kūlana Kūlana:
- Hoʻolālā ka mechamical: Nā bolts, Nā wilipū, a makemakeʻia nā rivets no ka hōʻuluʻuluʻana i nā'āpana A383.
- Arelay Kahi: Hiki ke hoʻohanaʻia nā'ōkuhi hoʻonohonoho e komo pū me nā'āpana me kaʻole o nā pilikia e pili ana i ka undering.
Nā kuhi kūikawā:
- Ināʻaʻole hikiʻole ke kala, hana kūikawā e like me ka friction stir crit (FSW) e noʻonoʻoʻia, Akā pono kēia i ka mālama pono.
Ke hoʻopauʻana i nā hana
Ke kālaiʻana a me ka polish:
- Hoʻohana e hoʻokō i kahi kūpono paulapua a iʻole e hoʻokaʻawale i nā hemahema ma hope o ka hoʻoleiʻana a iʻole machining.
- Koi pono e pale i ka paleʻana, hiki ke hōʻino i ka mea.
Deburing:
- Hoʻopau i nā kihi koʻikoʻi a iʻole nā burrs i waihoʻia mai ka machining a iʻole ke kāheaʻana.
- Hiki ke hanaʻia a hoʻohanaʻole paha i nā lako o nā automated.
6. Loaʻa iā A383 ma luna o nā mea make'ē aʻe
A383 alumini alloy hāʻawi i nā mea pono i kekahi mau mea nui ma mua o nā mea hana maʻamau maʻamau,
Ke hana nei ia i kahi koho i makemakeʻia no nā noi kūikawā e koi ana i ka cest chibors a me ke kū'ēʻana i nā hemahema. Ma lalo o nā pono kālā e hoʻonoho ai i A383 ma kahi e like me A380 a me A360.
ʻO ka Castability maikaʻi loa
- Low poroshity: ʻO A383 hōʻike i ka poosity haʻahaʻa haʻahaʻa i ka wā o ke kaʻina hana, hopena i ka denser a me nāʻano kani kani hou. Hoʻemi kēia i ka pilikia o nā hemahema e like me nā mea hana a iʻole nā pale.
- Nā hiʻohiʻona: ʻO ka alloy ka mea nui, Eʻae iā ia e hoʻopiha i nā'ōwili me nā geomera paʻakikī. ʻO kēia ka mea kūpono no ka hanaʻana i nā'āpana i nā'āpana a me nā'āpana kiko'ī.
- Hoʻemiʻia: A383 MIMIMIZES Shrikoge i ka wā e hoʻoponopono ai, Ke hōʻoia nei i ka pololei dimensional a me ka hōʻemiʻana i ka pono o ka post.
Hoʻopiliʻia ke kū'ēʻana
- Hoʻomaikaʻiʻia: Ua hoʻohālikelikeʻia i kekahi mau mea make, Hāʻawiʻo A383, kinopa, a me ka wai paʻakai.
ʻO kēia ka mea kūpono loa no nā noi marine a me nā noi waho. - Hoʻopau ʻili: ʻO kāna mau waiwai corrosion-resistant e hāʻawi i ka mālamaʻana i kahi mea maikaʻi e hoʻopau i ka manawa, ʻOiai ma nā kūlana Harsh.
Nā Pīkuhi Propertinies
- Ka ikaika ikaika-i-paona: Hāʻawiʻo A383 i kahi kaulike maikaʻi o ka ikaika a me nā hiʻohiʻona māmā,
Ke kūpono nei i nā noi i kahi e hōʻemi ai ka hōʻemiʻana o ka hōʻemiʻana me kaʻole o ka hoʻopiliʻana i nāʻano kūpono. - E kāʻei i ke kū'ē: Ke hōʻike nei ka Alyy i nā mea i hoʻopiliʻia e hoʻopiliʻia i nā pale i hoʻohālikelikeʻia e like me nā mea'ē aʻe e like me A380, e hoʻonui ana i kona longontity i loko o nā wahi kiʻekiʻe.
ʻO keʻano o ke kālepa a me ke kālepa
- ʻO ka wehe wela: Ua loaʻa iā A383, e kūpono ana i nā mea wela wela a me nā'āpana'ē aʻe e koi ai i ka hoʻokaʻawaleʻana i ka wela wela.
- Noi kelepona: He lawa keʻano o konaʻoihana uila no ka hoʻohanaʻana i nā mea e hoʻopili ai a me nā mea hou no nā polokalamu uila, Hāʻawi iā EMI (ʻO ka hoʻohui uila uila) kūlā.
Kumukūʻai-kūpono
- Mea kūponoʻole: Ua kūpono a383, Ke hana nei i kahi koho koho-kūpono no ka holo nuiʻana o ka hana nui.
- Hoʻemiʻia nā kumukūʻai o ka pou: Ma muli o kāna mau mea haʻahaʻa haʻahaʻa a me ka hoʻopau maikaʻi loa, Pono pinepineʻo A383 i nā hana kekona liʻiliʻi e like me ka polish a iʻole machining, ka mālamaʻana i ka manawa a me ke kālā.
Kū ponoʻole
- Nā mea paʻa paʻa: A383 mālama pono i ka hoʻomauʻana i ka lōʻihi o ka hanaʻana ma mua a ma hope o ke kaʻina hana, e hōʻoiaʻiʻo ana i nā'āpana kūpono a me ka hōʻemiʻana i ka hopena o ke kauaʻana a iʻole kaʻoluʻolu.
- ʻO ka hoʻokele hoʻokolokolo hoʻokolokolo: ʻO ka hoʻohanaʻana o ka alloy a alloy o ka expansion i kūpono i kūpono i nā noi i kūpono i nā mea e makemakeʻia.
ʻAno ʻano
- Laulā ākea o nā noi: Hiki ke hoʻohanaʻiaʻo A383 ma waena o nāʻoihana liʻiliʻi,
e komo pū me Automotive, mea uila, nā huahana kūʻai, a me nā mīkiniʻoihana, Mahalo i kāna hana a me ka hana kaulike. - Ka hoʻohālikelikeʻana me nā mālama kino: Ua kūpono ka alloy me nā hana likeʻole e like me nā mea e like me ka pauʻana, Kāleka, a me ka papahele, e hoʻopili ana i kāna hoʻopiʻi aesthetic a me nā hana.
7. Nā noi o A383 aluminum alloy
A383 aluminum alloy, ʻO kahi koho kaulana i kaʻoihana Die-Casting, i hoʻohana nuiʻia ma muli o kāna mau mea hana maikaʻi loa, Ke kū'ē neiʻo Corrosionion, a mālie o ka lawaiʻaʻana.
Aia ma lalo nei kekahi o nā noi nui o A383 alumini alloy ma waena o nāʻoihana likeʻole:
Ka Hoʻolālā Wīwī
- Na'Āpana Engine: Hoʻohana pinepineʻiaʻo A383 no ka hanaʻana i nā brackets mīkini, urowing,
a me nā wahi hana'ē aʻe ma muli o kona kiʻekiʻe kiʻekiʻe-kiʻekiʻe a me ka hiki ke kaupaona a me ka hiki ke loaʻa me ka mahana kiʻekiʻe. - Nā'ōnaehana transeles: Hoʻohanaʻia ia i nā hihia o ka hoʻounaʻana a me nā pale Valve ma muli o kānaʻano dimensional a me ke kū'ēʻana.
- Nā'āpana hoʻonohonoho: ʻO ka alloy ke kūpono no ka hanaʻana i nā kukui māmā a me nā mea e like me nā huila e like me nā huila, Nā'āpana Chassis, a me nā'ōnaehana hoʻoponopono.
Nā uila a me nāʻoihana uila
- Nā mea hoʻopuni a me nā houssings: A383's Finerment Electrowers (Emi) ʻO nā waiwai pale e kūpono ai ia uila nā mea hoʻopili, me nā mea no nā kamepiula, Nā'ōpala, a me nā lako kelepona.
- Sinks wela: ʻO kā lākou condalctivity a me nā kuʻekuʻe kuʻekuʻe i hana iā lākou i kahi koho maikaʻi loa no nā mea i hoʻokaʻawale i nā mea uila.

Nā huahana kūʻai
- Hale hana hale: Hoʻohana pinepineʻiaʻo A383 i ka hana o nā'āpana no ka holoiʻana i nā mīkini holoi, Mea Refigierats,
a me nā mea ea ea e pili ana i kona mau manawa a me ka paleʻana i nā kumu kūlohelohe. - Ke kukui uila: Hoʻohanaʻia ka alloy i ka hanaʻana o nā hale o ke kukui a me nā'āpana māmā ma muli o kona hoʻopiʻiʻana a me ka hiki ke mālama i keʻano.
Nā mīkini mīkini
- Pumps a me nā valves: Ua kūpono ke kū'ēʻo A3833, nā kino valve, a me nā'āpana'ē aʻe i hōʻikeʻia i nā mistiture a iʻole nā mea kanu.
- Nā mea pāʻani a me nā mea paʻa: ʻO ka Manchinenability a Alloy a me nā pale pale eʻaeʻia e hoʻohanaʻia ma nā wahi, Nā Kahu, nā bolts, a me nā mea hana paʻa'ē aʻe.
ʻO nā noi Marine
- Marine Nā Palaki'ā: ʻO ka paleʻana o A3833333, nā brackets, a me nā'āpana moku liʻiliʻi.
- Nā mea hana ma lalo: Hoʻohanaʻia ia ma lalo o nā mea e pili ana i nā mea leʻaleʻa a me nā hoʻopili no nā sensors a me nā lako'ē aʻe.
8. Nā pilikia a me nā palena
ʻOiaiʻo kāna mau pono, Loaʻa i ka A383 alumini alloy i kekahi mau palena e pili ana i nā mea hana e hoʻopili ai i kāna hana.
- Ikaika ikaika: Ua hoʻohālikelikeʻia i A380, Ua hōʻemiʻo A383 i ka ikaika a me ka ikaika, Hoʻopili i kāna hoʻohanaʻana i nā noi kiʻekiʻe. E uku paha nāʻenehana me nā hoʻolālā i hoʻoikaikaʻia.
- Hoʻemiʻia ka paʻakikī: Hoʻopili iki ka paʻakikī haʻahaʻa i nā pale i loko o nā wahi kiʻekiʻe. ʻO nā lako hana e like me ke anaodizing a iʻole nā lole e hiki ke hoʻonui i ka durability.
- Nā Kūlana Kūlana: Hiki i nā hana hana hana-paʻakikī a me ka hoʻohaʻahaʻa haʻahaʻa hiki ke hoʻokaʻawale i nā mea hana.
Ua kohoʻia nā'āpanaʻokiʻoki a me nā'ōnaehana kiʻekiʻe o ke kumukūʻai kiʻekiʻe e kōkua i kēia mau pilikia. - ʻO ke kaʻina hana: ʻOiaiʻo nā mea hana maikaʻi maikaʻi loa, ʻO ka mana kūpono o ka mahana o ka mahana a me nā uku hoʻoliʻiliʻi e koʻikoʻi e pale i nā hemahema e like me ka possity a me ka shrink.
Hoʻomaʻamaʻa nā'ōnaehana loiloi holomua. - Uku kiʻekiʻe: ʻOi aku ka nui o A383. Akā naʻe,, ʻO kona mau manawaleʻa a hōʻemi i nā pono mālama pono e kōkua i nā kumukūʻai mua o ka hana ma mua o ka manawa.
9. ʻO nā hiʻohiʻona hou a me nā makemakeʻole
- Holomua i loko o ka hānaiʻana: ʻO ka maʻalahi a me ka manawa maoli ka nānāʻana i ka hoʻomaikaʻiʻana i ka hana ma 20-30%, ka hoʻohālikelikeʻana i nā wikiwiki injection, nā wela wela, a me nā uku hōʻoluʻolu e hōʻemi ai i nā hemahema.
- Hoʻonui i nā hoʻololi hoʻololi: ʻO ka microtalloying me nā inoa inoaʻo Nano-Adduitives e hoʻonui i ka hana grain, Hoʻonui i ka ikaika o ka ikaika ma luna o 10% a ho'ēmi i ka huki wela i nā'āpana i nā'āpana.
- Hana Manaʻo: Hana ikaika-maikaʻi e hōʻemi ana i ka hōʻemiʻana i ka mana o ka mana e 15%,
ʻOiai e hoʻomaikaʻi hou i nā uku haʻahaʻa haʻahaʻa haʻahaʻa a me nā wāwae wāwae, ke kākoʻoʻana i nā pahuhopuʻo Global. - ʻO ka hana akamai akamai: It sussors and wasticictive encytics e hoʻoikaika i ka mana maikaʻi, hoʻemi i ka mīkini mīkini downtime e 25% a me ka hoʻomaikaʻiʻana i nā hana hana.
- Ke hoʻonui nei i ka noi mākeke: Me kahi hana 5.2% Cagr ma luna o nā makahiki e hiki mai ana,
Ke piʻi neiʻo A383 i kahi ORTOMOTITE, mea uila, a me nā noi pili hou, e alakaʻiʻia e nā mea māmā a me nā pono kūponoʻole.
10. Hoʻohālikelike hoʻohālikelike me nā alloys'ē aʻe
Aia ma lalo he papa hoʻohālikelike e hōʻike ana i nāʻokoʻa nui ma waena o A383 alumini alloy a me kekahi mau koho maʻamau i hoʻohanaʻia ma keʻano nui, e like me A380, A360, a adc12.
Kōkua kēia loiloi i ka hōʻikeʻana i nā mea kūikawā a38333.
| Waiwai | A383 | A380 | A360 | ADC12 |
|---|---|---|---|---|
| Ikaika ikaika (Mpa) | 310-325 | 310-325 | 317-330 | 300-320 |
| Ka ikaika (Mpa) | 150-160 | 160-170 | 160-175 | 155-165 |
| Kaulikeia | Kūpono; ʻoi aku ka nui o ka loli no ka paʻakikī, nā mea kūʻai i hoʻopaʻaʻia | Maikaʻi loa; lawa no nā noi maʻamau | Loli; Hoʻolālā no nā'āpana Corrosion-koʻikoʻi | Kūpono; hoʻohālikelike i A383 |
| Ke kū'ē neiʻo Corrosionion | High; hoʻomaikaʻiʻia ma muli o ka haʻahaʻa haʻahaʻa haʻahaʻa haʻahaʻa | Loli; kaulike akāʻaʻole i manaʻoʻia no nā wahi hoʻoponopono | High; maikaʻi loa no nā noi moana | Loli; like me A380 |
ʻO ka paleʻana i ke kū'ēʻana |
Luna loa; ʻO Microstruistarit Microstructure Minimizes | Loli; ʻoi aku ka nui o ka hoʻopiʻiʻana i nā'āpana likeʻole | Haʻahaʻa; ʻoi aku ka maikaʻi o ka hopuʻana i nāʻano paʻakikī | Hoʻohālikelike i A383 |
| Markinpalibility | Loli; hoʻomaikaʻiʻia i nā hana hana | Loli; ʻO ke kūlana no nā mea hana make | Kūpono; maʻalahi ka mīkini no nā'āpana kiʻekiʻe-pololei | Loli; like me A380 |
| Nā noi maʻamau | Kūlike, nā'āpana i hoʻopaʻaʻia i loko o nā kaʻa a me nā mea uila | ʻO ke kumu nui-ke kumu e kau ana i nā'āpana kaʻa a me nā'āpanaʻoihana | Marine a me nā noi a Corrosioni-koʻikoʻi | Nā mea hoʻohana uila a me nā mea kūʻai nui |
Nā Kūleʻa Kil:
- A383 Hono ʻO ka wai nui and ʻO ka paleʻana i ke kū'ēʻana, Ke kūpono nei i ka paʻakikī, nā hoʻolālā maikaʻiʻole. Hōʻike pūʻiaʻo ia i ka paleʻana o ka corrosioni ma muli o kānaʻano koho.
- A380 he kūpono no ka kumu nui-kumu e hānai ai, Akā e hakakā paha me ka huki wela i nā hoʻolālā intrigate i hoʻohālikelikeʻia i A383.
- A360 Hāʻawi i nā pale kū'ē maikaʻi loa, nui no nā wahi moana, akā,ʻaʻole i like ka hopena o ke kahe a me ka wela wela.
- ADC12, Ua hoʻohana nuiʻia ma nā mākeke Asia, hoʻolako i nā mea hoʻohālikelike i A383 me nā mea likeʻole, ʻOiaiʻaʻole paha e hāʻawi mau i ka pae like o ka paleʻana i ka pale.
11. Hopena
Ua puka maiʻo A383, ka hoʻohuiʻana i nā mea i hoʻonuiʻia, hoʻomaikaʻiʻia i ke kū'ē, a me nā mea pono kaulike.
Hāʻawi ia i keʻano o ka paleʻana i keʻano o ka paleʻana i ka paleʻana a me nā mea hoʻopihapiha maikaʻi loa, Ke kūpono nei i ka hoʻoikaikaʻana,
nā'āpana likeʻole ma waena o nāʻoihana e like me ka automotive, mea uila, a me nā lako hanaʻoihana.
Me nā mea hana hoʻomau ma ka hoʻololiʻana i ka hoʻololiʻana, Ke kaʻina hanaʻana, a me ka hoʻomaʻamaʻaʻana, Ua hoʻonohonohoʻiaʻo A383 e pāʻani i kahi hana koʻikoʻi nui i ka hana nui e hana ai.
LangHe ʻO ke koho kūpono kūpono no kāu hana e pono ai inā ponoʻoe i nā lawelawe kiʻekiʻe A3833 alumini.