He aha ka mea kiʻekiʻe e make ai (HPDC)?

Papa o nāʻikepili Hōʻike

1. Hōʻikeʻike

ʻO keʻano nui o ke koʻikoʻi (HPDC) kū i ka mua o ka hanaʻana i nā mea hana.

I HPDC, Loaʻa nāʻike i ka mīkini molten ma ke kaomiʻana i 200 Mpa i loko o kahi kila kila hou (make), ka loaʻaʻana o ka paʻakikī, kokoke-net-mode'āpana i kekona.

Mai konaʻoihanaʻana i ka makahiki 20 mau kenekulia ma mua o ka nui o ka alnuna mua a Alminim- a me nā mīkini wela-cang-cang i nā makahiki 1950,

Ua loaʻa iā HPDC i nāʻoihana hana mai Automotive i nā mea hoʻohana uila.

I kēia mau lā, ʻO ka mea e lawe ana i ka honua USD 60 'ōpū ALO, me ka palapala HPDC no ka luna 70 % o nā hale kūʻaiʻoleʻole.

Hōʻike kēiaʻatikala i nā loina o HPDC, Kahawai, mea waiwai, noi, a me nā keʻena e hiki mai ana, nā mea e hoʻopili ai i nāʻenehana a me nā hoʻoholo hoʻoholo me kaʻike hohonu i ke kaʻina hana.

2. He aha ka mea kiʻekiʻe e make ai?

Ke kiʻekiʻe kiʻekiʻe e hoʻolauna ana i nā pale i loko o nā pahu molten alloy i loko o kahi neʻeʻana i ka sholl i ka wikiwiki kiʻekiʻe a me ke kaomi.

ʻO kahi pana pana i kahi keʻena hoʻokūkū ikaika e hoʻoheheʻe i ka mea hao ma o kahi'ōnaehana gating i ka make. ʻO ka hydraulic a iʻole nā ​​mea hana i hoʻopaʻaʻia a laila clamp i nā mea make e kū'ē pū i nā pūʻali koa.

Ma hope o kahi manawa pōkole pōkole-pinepine wale nō 2-10 kekona-ʻO ka mīkini wehe, e hōʻole i ka mea kūʻai aku, E hōʻuluʻulu i nā mea waiwai nui, a hana hou i ka cycle i loko 20-60 kekona.

Ua loaʻaʻo HPDC i nā mea paʻa paʻa (± 0.05 mm) a me nā papa maikaʻi loa (RA 0.8-1.6 μm), Ke kūpono nei i ka hana kiʻekiʻe o ka māmā o ka māmā, nā mea hoʻohālikelike.

ʻO keʻano nui o ke koʻikoʻi
ʻO keʻano nui o ke koʻikoʻi

3. ʻO nā kumu kumu kumu o ke koʻikoʻi o ke kiʻekiʻe

Paulimalike & Nā Mulu Dcadick

Hoʻohuiʻo HPDC i ke kiʻekiʻe kiʻekiʻe (E.g., 700-780 ° C No ka alumini alloys) me ke koʻikoʻi kiʻekiʻe.

Ka wikiwiki o ka wikiwiki (a i 30 m / s) e hōʻoia i ka hoʻopiliʻana i ka hoʻopihaʻana i loko 20-50 ms, ho'ēmi i nā shuts anuanu.

ʻO nā mea hoʻolālā i nā mea kūʻai aku i nā mea kanu wahine (200-350 ° C)-ʻO nā'ōkuhi pale pale a pale aku i nā hemahema.

Hoʻolālāʻo Die: Goting, ʻAʻa, & Nā meaʻelele

Nā meaʻenehana e hoʻohālikelike i nā'ōnaehana geting-sprues, Nā meaʻelele, gates-no ka holoʻana o ka laminar. Waiho lākou i nā vents ma nā wahi kiʻekiʻe kiʻekiʻe e hoʻonui ai i ka ea a me nā hau.

Nā'āpana Runner kūpono (E.g., 10-50 mm² No ka alumini) E hōʻoia i ka hoʻololiʻana i nā manawa a hōʻemi i ka turbuglence.

Ka hoʻokeleʻana o Thermal: Hoʻohui & Ho'ōla

Hoʻohana pono i ka mana o ka Thermal i hoʻohana i nā channel a iʻole nā ​​mea e hoʻopili ai i nā pēpē e hoʻopili ai i ka wela ma 5-15 kw / o of Meld dire.

Make i nā mahana e kū ai a puni 200-250 ° C I ka wā o ka hana paʻa, Ke mālama nei i ka pono o ke ola a me ke ola holoʻokoʻa (50,000-200,000 mau hana).

4. ʻO keʻano nui o ke koʻikoʻi (HPDC) Kaʻina hana hana

Alloy mering and metal lapaʻau

Ka mua, loaʻa nā mea loaʻa i kahi inruction a iʻole ke ahi-ahi-ahi me ka hoʻomaʻemaʻe hoʻomaʻemaʻeʻana a iʻole recycled scrap.

ʻO kā lākou mau mahana e pili ana i nā hoʻonohonoho hoʻonohonoho alloy-kūikawā700 ° C No A380 Aluminim, 450 ° C No ka luna 3 zinc, Oole 650 ° C no Az91D Magnesium-Ke hoʻopaʻaʻia nei i loko o ± 5 ° C e hōʻoia i ka lawaʻana o ka nui.

I ka wā hana, Hoʻokumu nāʻenehana i nā papa papaʻai a iʻole ka hanaʻana i kahi balota o ka balota eʻoki i ka hydrogen, eʻoki ana i ka poosity e a 30 %.

Hoʻohui pū lākou i nā fluxes a iʻole nā ​​mea hana e hoʻoponopono ai i ka hoʻopiliʻana (E.g., E hōʻoluʻolu i ka silika i ka alumini i 7 % No ka mea e hoʻopiha maikaʻi ai) Ma mua o ka skimming dross mai ka pā o ka umu.

Ke kiʻekiʻe kiʻekiʻe e hoʻomoʻa ana i ke kaʻina hana
ʻO ke kaʻina hana nui

ʻO Shot-Piston Mechanism: Anuanu- vsa. Nā Pūnaewele Honu Honu Hod

A hiki, ʻO ke kaʻina hana e pili ana i ka alloy:

  • Anuʻi-chance hpdc
    • Loaʻa i nā mea hana kīwī i kālaiʻia i loko o ka wai wai-wai.
    • ʻO kahi piston driven driton a laila e hoʻopau i ka mea hao ma o ka gooseneck a i ka make.
    • ʻO nā mea hoʻoponopono nui o kēia hoʻonohonohoʻana (aluminum, keleawe) a pana i nā helu mai 50 i 2,000 cm³.
  • Kahu Hot-CHBIR hpdc
    • ʻO nā mea i hoʻopiliʻia i loko o ka metmers i loko o ka melt.
    • Hoʻokomoʻia kahi plunger i nā mea hao i loko o ke keʻena a laila ua hanaʻo ia i ka make.
    • Zinc a me ka magnesium alloys-melting ma lalo nei 450 ° C-Fill iniha a hiki i 200 cm³ Me nā manawa pāʻani ma lalo 20 S.

Hoʻokumu nā'ōnaehanaʻelua i nā wikiwiki 10-30 m / s a me nā mea hana kūpono o 10-100 mPA E kiʻi i nā hiʻohiʻona maikaʻi a me ka uku no ka shrinkage.

Hoʻopili i nā dynamics hoʻopihapiha: Hoʻololi, Inteisefication, a hoʻopaʻa paʻa

Ke hoʻomaka nei ka pana pana i kāna stroke, ʻO ke kaheʻana o nā mea hao ma o ka'ōnaehana gating i loko o ka wai make.

Hoʻolālā nā mīkini hana i nā mea holo a me nā'īpuka-pinepine 10-50 mm² Kāne-'āpana- e hoʻolaha Lamini, ʻO ka ho'ēmiʻana i ka turbulence a me ka mea e hoʻopili aiʻo Oxide.

Koke koke, Hoʻopili ka mīkini i kahi hoʻoikaika a iʻole ka hoʻopaʻaʻana i ka ikaika no 2-5 kekona.

Ke hana nei kēia hana i nā mea kilokilo hou i loko o nā'āpana hana a me nā mea kūʻai aku e like me nā mea kūʻai aku e like me ka mea kūʻai aku.

Conform chancels channels ma ka make i ka wela wela i 15 Kw / o, kuhikuhiʻana i ka hoʻoponoponoʻana mai nā iwi liʻiliʻi i loko i loko o nā mea nui a me ka hope loa i nā alaloa.

Email, Ho'ākāka, a me ka hanaʻana i ka hanaʻana

NA MEA Kūpuia-Typically 2-10 kekona No ka hapanui o nā pā alumini. Ejector Charary a laila kaomi i ka'āpana manuahi, a ua paniʻia ka mīkini no ka pōkole aʻe.

I kēia manawa, ʻO ka Raw Canting Canding Gates, Nā meaʻelele, a me ka uila. ʻO nā kiʻina Trim automated a iʻole cnc saw e wehe i kēia mau hiʻohiʻona i loko 5-15 kekona, e hoʻoponopono hou ana 90 % o ka mea nui o ka mea nui no ka remot.

Hope loa, nā'āpana paha i lalo o ka panaʻana, CNC makiʻi o nā papa koʻikoʻi (i ± 0.02 mm), a me nā hana wela wela-like t6 iging at 155 ° C-ʻO ka OPTIMIZIZIZE MONECIANES ma mua o ka hoʻounaʻana.

5. ʻO ka nui o nā mea e hoʻomoʻa ana i ka hanaʻana

ʻO keʻano nui o ke koʻikoʻi (HPDC) ʻO nā mea maikaʻi me nā mea āpau non-ferrous e hui pū ai, ikaika, a me ke kū'ēʻana.

Hōʻike pinepine nāʻenehana i nā Alumini, zinc, a me nā mea hana magnesium no ka HPDC-ʻO kēlā me kēiaʻohana e hāʻawi i nā waiwai i hāʻawiʻia a me nā hana noi.

ʻO nā'āpana kiʻekiʻe e hānai ana i nā'āpana aluminim
ʻO nā'āpana kiʻekiʻe e hānai ana i nā'āpana aluminim

Apana Apana Aluminum

Aluminum e hoʻohanohano iā HPDC no kāna māmā māmā, ʻO ka ikaika maikaʻi, and Ke kū'ē neiʻo Corrosionion. ʻEkolu mau helu heluʻekolu:

A380

  • Ka Hoʻolālā: 9-12 % A, 3-4 % Cu, 0.5 % Mg, kaulike al
  • Hoʻohemo melū: 580-640 ° C
  • Huakai: 2.65 g / cm³
  • Ikaika ikaika: 260-300 mPA
  • Ewangantion: 2-5 %
  • Noi: ʻO nā Brackets Engine Engine Engine, nā hale paʻi kiʻi, Nā kino kino

A356

  • Ka Hoʻolālā: 6-7 % A, 0.3 % Mg, Trace Fe / cu, kaulike al
  • Hoʻohemo melū: 600-650 ° C
  • Huakai: 2.68 g / cm³
  • Ikaika ikaika (T6): 300-350 mpa
  • Ewangantion (T6): 7-10 %
  • Noi: ʻO nā leʻaleʻa wela, Nā Kūlana Kūʻai Arosspace, I alakaʻiʻia i ka wai wela

ADC12 (ʻO iaʻo ia)

  • Ka Hoʻolālā: 10-13 % A, 2-3 % Cu, 0.5 % Mg, kaulike al
  • Hoʻohemo melū: 575-635 ° C
  • Huakai: 2.68 g / cm³
  • Ikaika ikaika: 230-270 mpa
  • Ewangantion: 2-4 %
  • Noi: Nā mea hoʻohui uila, Nā'āpana hana, make-nā huila

ZINC Alloys

Hāʻawiʻo Zinc Alloys ʻO keʻano kiʻekiʻe kiʻekiʻe loa and ʻO ka'ōlelo kiko'ī maikaʻi loa ma nā haʻahaʻa haʻahaʻa haʻahaʻa. Hoʻokomoʻia nā kiʻi nui:

na kaumaha 3

  • Ka Hoʻolālā: 4 % AL, 0.04 % Mg, 0.03 % Cu, kaulike zn
  • Malting Point: ~ 385 ° C
  • Huakai: 6.6 g / cm³
  • Ikaika ikaika: 280 Mpa
  • Ewangantion: 2 %
  • Noi: Nāʻuala maikaʻi, liʻiliʻi liʻiliʻi'enekino liʻiliʻi, nā pilina pili

na kaumaha 5

  • Ka Hoʻolālā: 1 % AL, 0.1 % Mg, 0.7 % Cu, kaulike zn
  • Malting Point: ~ 390 ° C
  • Huakai: 6.7 g / cm³
  • Ikaika ikaika: 310 Mpa
  • Ewangantion: 1.5 %
  • Noi: Nā mea paʻaʻole-resistant, Kālā palekana, Nā Laki

MAKENESIM ALLOYS

Hāʻawiʻo Magnesium Alloys i ka ʻO keʻano kūlohelohe māmā a me nā waiwai maikaʻi maikaʻi. Komo nā helu nui:

AZ91D

  • Ka Hoʻolālā: 9 % AL, 1 % Zn, 0.2 % Mn, Kālā MG
  • Hoʻohemo melū: 630-650 ° C
  • Huakai: 1.81 g / cm³
  • Ikaika ikaika: 200 Mpa
  • Ewangantion: 2 %
  • Noi: Nā Huakuai Mīkini, nā kino, ʻO nā huila kaʻa kaʻa kaʻa kaʻa o Automotive

AM60B

  • Ka Hoʻolālā: 6 % AL, 0.13 % Mn, Kālā MG
  • Hoʻohemo melū: 615-635 ° C
  • Huakai: 1.78 g / cm³
  • Ikaika ikaika: 240 Mpa
  • Ewangantion: 7 %
  • Noi: Nā pale kūlokoʻo Aerosopa, nā lako hāmeʻa, ʻO nā'āpana kukui māmā

E puka mai ana & HE MAU LOA HOOLAHA

ʻO nā mea hou aku i ka HPDC HPDC i loko o nāʻano kūlana kiʻekiʻe:

Sillicon-Lawe Aluminum (E.g., Silafornt-36)

  • Inā kaʻike: ~ 36 % No ka hoʻonuiʻana i ka hoʻonuiʻana
  • Noi: Nā poloka mīkini, nā poʻo cylinder me ka leʻaleʻa liʻiliʻi

ʻO nā leka uila metala semi-solid

  • Ke heleʻana ma waena o nā wai a me nā mea paʻa e hōʻemi i ka pososity a hoʻomaikaʻi i nā waiwai mechanical, ʻoi aku i loko o nā hoʻolālā kiʻekiʻe.

6. Loaʻa & Nā palena o keʻano nui o ke koʻikoʻi

'Olununi High-kaomiʻana i ke kaomiʻana i ka hale o ka hoʻokele kaʻa
'Olununi High-kaomiʻana i ke kaomiʻana i ka hale o ka hoʻokele kaʻa

Loaʻa

ʻO ka wikiwiki wikiwiki

Ma ka hoʻopiliʻana i nā mea hao molten ma ke kaomiʻana a hiki i 200 Mpa, Hoʻopihaʻo HPDC a hoʻopau i nā'āpana i kahi liʻiliʻi e like me 20-60 kekona I kēlā me kēia.

NOEHUI, Hiki i kahi mīkini hoʻokahi ke hana 1,000+ nā brackets liʻiliʻi alumiinum no ka hoʻololiʻana, ka ho'ēmiʻana i nā manawa alakaʻi i hoʻohālikelikeʻia i ke one a iʻole ka hoʻopukaʻana.

ʻOkoʻaʻokoʻa

Ka huiʻana o ka huiʻana o ka hana i hanaʻia a me nā mea kiʻekiʻe a me ke kiʻekiʻe-wikiwiki e hoʻopiha i nā mea i hāʻawiʻia e like me ka paʻa ± 0.02-0.05 mm.

Ma ka hopena, nā'āpana pinepine e koi wale 0.2-0.5 mm o ka machining stock-up a i 40 % ua emi iho ma mua o ka gravity-stervistants e hōʻemi i nā mea i hōʻemiʻia a me ka hana hana.

ʻO nā'āpana pālopa

ʻO nā mea hoʻokūkū kiʻekiʻe o HPDC 0.5 mm I Zinc alloys a 1 mm I loko o nā alluinum a Alminim.

Kākoʻo kēia hiki i kēia mau hoʻolālā māmā 10-20 %-ʻO ka hoʻomaʻamaʻaʻana i ka hoʻohuiʻana o nā mea i hoʻopiliʻia (E.g., nā mea paʻa) I kahi hana hoʻokahi.

Ke hoʻopauʻana i ke kiʻekiʻe

Make i nā papa hana RA 0.8-1.6 μm e hoʻoneʻe pololei i ka maikaʻi i ka mālamaʻana, pinepine pinepine e hoʻopau i ka decuring lua a iʻole ka polish.

E hoʻomaikaʻi houʻia kēlā mau holomua wikiwiki i ka hoʻopiliʻana i ka hoʻopiliʻana a hōʻemi i ka pilikia o ka corrossion.

Keʻano o ka mīkini kiʻekiʻe

Rapid, Hoʻopili i ka hoʻopihapiha hoʻopihapiha a hoʻopaʻaʻia i ka mana o ka microstructure maikaʻi me ka miosity liʻiliʻi.

ʻo kahi laʻana, Hiki iā A380 alumini nā mea hoʻokele a Aimminim e hiki i nā ikaika o nā 260-300 mPA a me elangations o 3-5 %, ʻO nā'āpana he nui.

Ka hana leak-paʻa

No ka mea,ʻo HPDC no nā metala i loko o nā lua ma lalo o ke kaomi kiʻekiʻe, Hōʻikeʻo Castles i kahi kokoke-zero permeility.

Hana kēia waiwai i ke kaʻina kūpono no nā hale o Hydraulic, nā kino valve, a me nā mea e pili ana i nā mea hana'ē aʻe.

ʻOtometi & Nā hana hana

Hoʻokomoʻia nā laina HPD FRYC e hoʻohui i nā'āpana robotic, Nā Kūlana Trimming, a me ka nānāʻana i ka laina, hoʻokō a hiki i 80 % Ka hōʻemiʻana i ka hana manual.

E hōʻoia i ka manawa kūpono i nā manawa maʻamau a me ka maikaʻi hou, Ke hoʻokele nei i nā uku hana ma kēlā me kēia.

PAHUI

ʻO nā mea kōkua kōkua kiʻekiʻe

He make nui no ka uku o HPDC maʻamau USD 20,000-150,000, me nā manawa alakaʻi o 6-12 mau pule.

No ka holoʻana i lalo 5,000 Nā'āpana, Hiki i kēia mau uku o nā kumukūʻai i waho e loaʻa i ka hana o ke kaʻina hana.

Alloy a me nā mea hana geometry

Hpdc sexls me alumini, zinc, a me nā mea nui magnesium akā hana i ka paʻakikī me nā metala kiʻekiʻe-mering-point (Kukui Kekuhi, keleawe) Ma muli o ka mold erosion a me ka momona o ka thermal.

Eia hou, ʻO nā mea paʻakikī, nā hale kūloko kūloko, a me nā mea e pono ai nā pale i nā pale i koi pinepineʻia i nā cores a iʻole nā ​​hui lehulehu, hoʻohui i ka hoʻolālā hoʻolālā a me ke kumukūʻai.

ʻO nā pōkā a me nā'āpana komo

ʻOiaiʻo HPDC Minorizies i hoʻohālikelikeʻia i nā hana gravity, Hiki i ka wikiwiki kiʻekiʻe ke kīleʻaleʻa i ka lewa a me nā orides ināʻaʻole i hoʻohālikelikeʻiaʻo Goneting.

Ke nānā pono nei (E.g., thermoleples, nā naʻau ikaika) E hoʻomau i ka mea pono eʻike a pololei i nā pilikia pososity.

ʻOihana Hoʻohuiʻoihana & Mālama

Hui pū nā mīkini hpdc i nā hydraulics, Pnuimatika, a me nā'ōnaehana kiʻekiʻe-kiʻekiʻe.

Ma ka hopena, koi lākou i nā mana pale pale 10,000-20,000 nā cens-to relalibrate i nā profile injection, Hoʻopili i nā hōʻailona, a me nā mea hoʻoponopono refurbish, ka hoʻohuiʻana i nā mea hana ma luna.

Kaupalenaʻia nā'āpana

ʻOiai maikaʻi no nā'āpana liʻiliʻi i waena o nā'āpana waena (ʻO nā mea liʻiliʻi a ~ 10 kg), Ua uluʻo HPDC i ka liʻiliʻi o ka hoʻokele waiwai nui (> 20 kg) Ma muli o nā manawa paʻakikī hou a me nā kiʻekiʻe o nā'āpana i loko,

kahi e hele ai ka Sanding Single i nā ala haʻahaʻa a haʻahaʻa paha e hōʻoia hou.

7. Nā noi o ke kumu nui e make ana

Ka Hoʻolālā Wīwī

  • Nā hale paʻi kiʻi
  • Nā kikowaena mīkini & Nā Hale Hōʻikeʻike
  • ʻO ka hoʻokeleʻana & Nā'āpana i hoʻokuʻuʻia
ʻO ka nui o nā kaumaha e hoʻomoʻa ana i nā'āpana zamak3 mau'āpana
ʻO ka nui o nā kaumaha e hoʻomoʻa ana i nā'āpana zamak3 mau'āpana

Mea uila & Nā hana hana

  • Nā Chassis Chassis & Nā kiʻi kelepona
  • I alakaʻiʻia i ka wai wela & Ka mana hoʻolakoʻia
  • ʻO nā mea uila home

Aerospace

  • Nā pale lole & Nā poloka mauna
  • Nā mea hana hana & Nā lāʻau-nā lāʻau
  • Ke kaʻa kaʻa kaʻaʻole (UAV) Nā Frame

Nā Pūnaewele Pūnaewele & ʻO nā mea kūpono loa

  • ʻO nā mea hana kiʻi kiʻi
  • Nā mea kūʻai aku
  • ʻO ka laweʻana i ka cludid inifollds

8. Nā mea hana a me nā mea hana o ke kiʻekiʻe kiʻekiʻe

ʻO keʻano nui o ke koʻikoʻi (HPDC) koi aku i nā mea mīkini i hana a me nā mea hana kūpono e harness i kona wikiwiki a me ka pololei.

Mai ka koho o nā papa mīkini i ka hoʻolālā a me ka upkeep o nā mea kila, Pāʻani kēlā me kēia mea i kahi hana pivotal i kahi kūpono, manawa manawa, a me ka nui o ke kumukūʻai o ka waiwai.

Ma lalo, E kiko'ī mākou i nā mea kūʻai nui a me nā mea noʻonoʻo e noʻonoʻo ai no nā hana HPDC.

Make i nā mea e kau ana i nāʻano mīkini

Ua hāʻule nā ​​mīkini HPDC iʻelua mau papa papa mua, hoʻokaʻawaleʻia e ko lākou mau mechanms a me nā mea hiki:

Nāʻano mīkini Pana leo (cm³) Clamping ikaika (k kn) Maikai no
Keʻa 100 - 2,000 500 - 5,000 Aluminum, Nā pāpale keleawe
'-Lelo wela 20 - 200 200 - 1,000 Zinc, MAKENESIM ALLOYS
  • Nā Pūnaewele maloʻo anu koi aku i ka hanaʻana o waho o nā mea hao molten i loko o kahi manamana wāwae.
    Ko lākou noho kiʻekiʻe kiʻekiʻe (a i 800 ° C) hoʻolilo iā lākou no nā allusum a me nā mea kūʻai aku.
  • Nā Pūnaewele Honu Honu Hod Hoʻopili i ka mechanism injection i loko o ka melt, e hiki i nā manawa pōkole e like me ka pōkole 15-30 kekona No nā'āpana zinc akā hoʻohana i ka hoʻohanaʻana i nā alloys haʻahaʻa haʻahaʻa (< 450 ° C).

Hoʻolālā i ka hāmū

Kūleʻa kūleʻa kūleʻa i hoʻolālā i ka hanaʻana i ka hanaʻana me ka mana o ka Thermal:

  1. Material Selection: Hōʻike nā meaʻenehana e like me H13 Oole 2344 no kā lākou huiʻana o ka paʻakikī (48-52 HRC) a me ka paleʻana i ka momona momona.
  2. KOMaiwai castucits: Conformal cooting-pinepine maopopo ma o mea hoʻohuiʻaha-E 10-20 kw / o o ka wela, e hōʻemi ana i ka manawa pōkole e 20 % a ho'ēmi i nā wahi wela wela.
  3. Goting & Kūhewaʻi: ʻO nā'āpana kūhelu pūnaewele (10-50 mm² no alumini) a me nā micro-vents (0.2-0.5 mm) E hōʻoia i ka hoʻopihaʻana o Paminar i kahi pakeleʻo RAPID, ho'ēmiʻana i ka pososity.
  4. Draft & Parting Lines: Hoʻohuiʻia nā Designers 1-3 ° Hoʻokomoʻia nā kihi a me nā hoʻolālā i waiho i nā laina e hoʻokaʻawale i ka ejection a pale i ka uila.

E nā simulation moll, hiki i nā hui ke koho i nā mea hoʻopiha piha a me ka hoʻoponopono, Ke kaʻa nei i nā kumukūʻai kūleʻa mua ma mua 90 %.

Make mea hana, Nā pāpale, a me ka mālama

He uku uku USD 20,000-150,000 Akā hiki ke hana 50,000-200,000 ʻO nā hale hoʻokipa me ka mālama kūpono. Hoʻohuiʻia nā hana koʻikoʻi:

  • Nāwaimaka: Nā lole pale (kiʻi kiʻi a zircon-e pili ana) e hoʻolōʻihi i ka ola make ma muli o ka hōʻemiʻana i ka absam.
    Nā helu noi o 10-30 μm hahau i ka kaulike ma waena o ka hoʻokuʻuʻana i ka hana a me ka dimensional kiʻekiʻe.
  • ʻO ka hoʻopololei & Relarbishment: Papa i hoʻonohonohoʻia 10,000-20,000 E hoʻihoʻi hou i nā SHOTS (Ra < 0.8 }m), Ke kākoʻo nei i kaʻike likeʻole.
  • ʻO ka hoʻokele CYCHEAL CYCLEL: ʻO ka nānāʻana i ka mahana o ka mahana (Thermocoups i nā mea make make) a hoʻopaʻaʻia i nā alaloa prehalat (200-350 ° C) Kāohi i ka checking a me ka hana kolohe ma ke kila kila.

E hoʻopili ana i kahi hoʻolālā mālama ikaika e pale i ka hoʻolālāʻana i ka downtimed e like me ka 30-50 % a mālama i nā mea kanu i luna o nā holo lōʻihi lōʻihi.

Hoʻohui a me nā hoʻohui hoʻohui

ʻO nā laina HPDC hou i nā auteraget ittation e hoʻoikaika ai i ka huahana a me ka pono:

  • ʻO ka nininiʻana o Robotic & Pana lima: ʻO nā Ladles a iʻole nā ​​kāwele i ka synchronize i ka wela a me ka manawa, ʻO ka hoʻemiʻana i nā hewa kanaka i ka laweʻana i ka hoʻoiliʻana.
  • Māhele Leki & Hoʻololi: Hoʻokomoʻia nā robots i nā hale kūʻai wela, e hoʻokaʻawale iā lākou i nā pihi Trim, a hoʻouka iā lākou i loko o ka nānāʻana i nā manawa hoʻokūkū 30 kekona.
  • In-line kūpono: Hoʻohui i nā'ōnaehanaʻike a me nā'āpana x-ray iʻikeʻia i nā mea i hoʻopaʻaʻia a i loko o ka possity kūloko a i loko o ka manawa maoli, Hoʻopā i nā hana hoʻoponopono koke.

Ma ka paniʻana i ka'ōlelo hoihoi ma waena o nā sensor mīkini, make data kūlana, a me nā mea hana hoʻolālā,
hoʻokō nā mea hana ʻO nā pono hana kūpono (Huoma) Nā luna 85 %-ʻO ka manaʻo koʻikoʻi i kaʻoihana 4.0 nā wahi.

9. O ka kūlana & Hōʻoia

Ka mālamaʻana i ka maikaʻi kūʻokoʻa ma ke kiʻekiʻe kiʻekiʻe e make ai i nā hinges e lele ana ma luna o nā pale defect defect, Ke nānā nei i ka hana maoli, a me nā mea hōʻike nānā ponoʻole.

'Olununi High-kaomiʻana i keʻano o ka ukiukiʻana i ka e-cheating
ʻO ke ala kiʻekiʻeʻo Alminimum

Nā hewa maʻamau a me ko lākou mitigation

Hewa ole Kumu Kāohi Kūʻai
ʻO ka pololi Dissolved hydrogen a iʻole ke komoʻana i ka ea ea i ka wā e hoʻopiha ai E hoʻohana i ka rotary det; E hoʻohālikelike i ka hoʻolālā puka no ka holoʻana o ka Laminar
ʻO nā leo shrink Ka hanaʻoleʻana i ka hanaʻana i nā mea hao E hoʻohui i ka intelisfication kūloko; ʻO ka mea i kū mai i nā'āpana nui
Nā'ōpū anuanu ʻO ka hoʻokaʻawaleʻana i ke kala kalaʻole a iʻole ka hoʻohaʻahaʻa haʻahaʻa Hoʻonui i ka wikiwiki (> 20 m / s); make make > 200 ° C
Pū uilani ʻAʻole lawa ka makeʻana o ka ikaika clamping Callibrate clamp cylinders (maʻamau 1.0-1.5 kn / cm²)
'Āʻia wela ʻO ke kaumaha o ke kaumaha ma luna o nā wahi ākea a iʻole nā ​​mea paʻa Hoʻopau i nā hoʻololiʻana o ka pā pōhaku; E hoʻohui i nā channels channing
Kuni bulu & Mau wele Make a make paha Hoʻopau i ka hanaʻana i ka make make o ka make

Ke nānā nei i ka hana maoli

Hoʻopili i nā meaʻike a me nā kumuwaiwai e hiki ai i ka mana o ka mana:

  • Shot-sraeve thermocoums: E nānā i ka wela ma keʻano o keʻano (± 2 ° C) No ka hōʻoia pono i ka nui.
  • Nā mea kūʻai aku: E hoʻopaʻa i ka hoʻoikaika ikaika (10-100 mPA) I ka make e hōʻoia i ka hanaʻana i ka hana.
  • Nā kāmera kiʻekiʻe: Hopu i nā hanana e hoʻopiha i nā hanana i 1,000 FPS, e hōʻike ana i ka turbulence a iʻole ke kauʻana i ke aniani.
  • ʻO nā kākā lāʻau paʻa: ʻO ka nānāʻana i ka weheʻana i ka wehe / pani a pani a pana aku i nā manawa eʻike ai i nā hana hoʻopunipuni e hoʻoponopono ai i nā hemahema.

Hoʻopili i kēia mau pahu i nā kahe i loko o kahiʻoihana 4.0 ʻO nā mea hana a Dashboard e hana i waho o nā kūlana i waho.

ʻO ka hōʻike hoʻokaumahaʻole (Ndt)

ʻO nā hana NDT i hōʻoia i ka pono kūloko i loko me kaʻole o nā'āpana hōʻino:

  • X-Kahī Piʻi: E hoʻomaopopo i ka postity subsurface (> 0.5 mm) a me nā manaʻo i loko o nā hale paʻahao.
  • ʻO ka ho'āʻoʻana: E nānā i nā faws braws a me nā waimaka wela; Hōʻike ka naʻau 0.2 mm resetian in alumini.
  • Dye-penenuant nānā: Nā hiʻohiʻona a iʻole nā ​​aniani i nā wahi i nā wahi hōʻailona koʻikoʻi.
  • ʻO ka ho'āʻoʻanaʻo Eddy-i kēia manawa: Loiloi i nāʻano paʻakikī paʻakikī a me nā'āpana micro-cracks i nā paiaʻili.

Loaʻa pinepine nā hanana i ka 5-10 % nā'āpana no 100 % Ndt i ka wā e hoʻolako ai i ka palekana o ka palekana a me nā mea olakino.

10. Hoʻohālikelike me nā hana kūʻai'ē aʻe

ʻO keʻano nui o ke koʻikoʻi (HPDC) noho i kahi papa hana likeʻole ma waena o nāʻenehana hana metala.

Ma ka hoʻohālikelikeʻana iā HPDC me ʻO ka mālamaʻana i ka nui, ʻO ka haʻahaʻa haʻahaʻa haʻahaʻa, and Kāhaka kūʻai kūʻai, Hiki iā mākou ke kuhikuhi i nā ikaika a me ke kālepaʻana o kēlā me kēia kaʻina hana-a kōkua i nāʻenehana e koho i keʻano kūpono no kā lākou mau'āpana.

ʻO ka nui o ke koʻikoʻi e hānai ana i ke kauʻana ma mua. ʻO ka mālamaʻana i ka nui

Pili HPDC ʻO ka mālamaʻana i ka nui
E hoʻopiha i ka mīkini Inihaʻia ma lalo o 10-200 mPA Nininiʻia e ka gravity wale nō (1 g)
Manawa manawa 20-60 s 60-180 s
Pilenawinui 0.5-3 mm ≥ 3 mm
Aiko ± 0.02-0.05 mm ± 0.1-0.5 mm
Hoʻopau ʻili RA 0.8-1.6 μm Ra 1.6-3.2 μm
Mea kūʻai & Ola $20 K -150 K; 50 K-200 K Loa Loa $5 K -50 k; 500-2 000 Nā Pāʻani Pūnaewele
Maikai no Ka nui, 'ōnē, nā'āpana likeʻole Palapala Kahiko, Nā'āpana Thuker, SMALER SOLTHER SILETH

Insight: ʻO HPDC Injects i ka metala ma ke kaomi kiʻekiʻe e hoʻokō ai i nā paia o nā paia a me nā mea kanu, ʻOiai ke kūʻai aku nei i nā mea kūʻai aku i ka wikiwiki a me nā kiko'ī no nā kumukūʻai haʻahaʻa haʻahaʻa a me nā mīkini maʻalahi.

ʻO keʻano nui o ke koʻikoʻi (HPDC) vsa. ʻO ka haʻahaʻa haʻahaʻa haʻahaʻa (Lpdc)

Pili HPDC Lpdc
Pae kiʻekiʻe 10-200 mPA 0.3-1.5 Bar
Kaho kahe Hoʻopiha piha me ka turbuglence Lohi, Hoʻopaʻa ka mana i nā minimizes turbulence
Potiwale Haʻahaʻa-medium (pono nā mea i kohoʻia) Haʻahaʻa loa (E hoʻopihapiha paʻa e hōʻemi i ka hoʻokomoʻana)
ʻO ka pā o ka paia Kūpono (a lalo i 0.5 mm) Maikaʻi loa (≥ 2 mm)
Manawa manawa 20-60 s 60-120 s
Mea paʻakikī High ('Clelo pololei, conformila ho'ōla) Loli (Hoʻolālā'Oiohoʻomaina'Āina maʻalahi)
Maikai no Mea paʻakikī, ʻO nā'āpana kiʻekiʻe kiʻekiʻe-wanana Nui, nā'āpana koʻikoʻi koʻikoʻi me nā koi haʻahaʻa haʻahaʻa

Insight: Hāʻawiʻo LPDC i ka mana o keʻano o ka paleʻana a me ka hoʻopihaʻana, Ke kūpono nei ia no nā mea hoʻonohonoho hoʻonohonoho, Ma heaʻo HPDC Excel ma nā paia o nā pā a me nā pā kiʻekiʻe.

ʻO ka nui o ke koʻikoʻi e hānai ana i ke kauʻana ma mua. Hoʻolei kālā

Pili HPDC Hoʻolei kālā
ʻAno mods Ua makeʻo Steeel Steel Hoʻokahi manawa hana
Kiko'ī & Huanui High, akā ua palena iki Nā kiʻekiʻe kiʻekiʻe loa, ʻO nā geometries manik
Hoʻopau ʻili RA 0.8-1.6 μm RA 0.8-3.2 μm
Aiko ± 0.02-0.05 mm ± 0.05-0.1 mm
Mea kūʻai & Ka manawa o waena o ka hoʻomaka a i ka wā pau High ($20 K -150 K; 6-12 mau pule) ʻOluʻolu-kiʻekiʻe ($5 K -50 k; 2-4 mau pule)
Manawa manawa 20-60 s 24-48 h no kēlā me kēia batch
Maikai no Nui loa, nā'āpana'āpana Hoʻohaʻahaʻa- i ka medium-volume, nā'āpana kiko'ī loa

Insight: ʻO ka kūʻaiʻana i ka waiwai kūʻai akuʻana i nā kikowaena HPDC ma Geometc ma Geometric paʻakikī a me nā kāpena liʻiliʻi liʻiliʻi. Akā naʻe,, Hāʻawiʻo HPDC i nā manawa pōkole pōkole pōkole a me nā uku haʻahaʻa ma lalo o nā kumukūʻai.

11. Hopena

ʻO ka wikiwiki kiʻekiʻe e hānai ai i ka laweʻana i ka wikiwiki, 'Clelo pololei, a me ke kumukūʻai-kūpono no nā mea waiwaiʻoleʻole i kēia hana hoʻokūkū i kēia lā.

Ma ka hakuʻana i kāna mau thermodynamics, Hoʻolālāʻo Die, Nāʻano hana, a me nā manawa kūpono, Hiki i nā meaʻenehana ke hana i ka HPDC e hoʻopuka i ka māmā, ʻO nā'āpana hana kiʻekiʻe ma ke kāʻei.

E like me ka simulation simulation a me nā mea hoʻohui hoʻohui, E hoʻomau ka HPDC e hele ana i ka neʻeʻana-hoʻoponopono i kona hana hoʻolālā ma waena o ka automotive, AerERPPACE, mea uila, a ma waho aʻe.

A ʻOihana Pūnaewele, Kū mākou i ka hui pū meʻoe i ka hoʻokuʻuʻana i kēia mau loea holomua e hoʻomaikaʻi i kāu mau hoʻolālā hoʻonohonoho, Koho Koho, Apia hanaa.

Ke hōʻoia nei eʻoi aku ka maikaʻi o kāu papahana eʻoi aku i kēlā me kēia hana a me nā mea hoʻokele.

Kāhea iā mākou i kēia lā!

 

FaqS

He aha nā mea hana maʻamau a me nā wahi e hoʻopau ai i ka hpdc e hoʻokō?

  • Nā mea hana dimensional: ± 0.02-0.05 mm
  • Paulapua: RA 0.8-1.6 μm

No ke aha e koʻikoʻi ai nā channel e hoʻomaʻemaʻe ai?

Conformal colting-pinepine 3d-paʻiʻia i loko o ka make-lawe i ka wai wela, e hōʻemi ana i nā manawa like ma luna o 20 %, Ke hōʻemi nei i ke kaumaha weliweli, a e hōʻoia i ka'āpana maʻamau i ka lōʻihi o ka holo lōʻihi (50,000+ Nā Pāʻani Pūnaewele).

He aha nā palena nui o HPDC?

  • ʻO ke kumukūʻai kōkua kiʻekiʻe ($20 000-150 000 e ka)
  • Nā palena'ē aʻe (palena i ka alumini, zinc, Magnesum)
  • Hoʻolālā Conants No nā'āpana hohonu hohonu a iʻole nāʻano ākea ākea ākea

'Aluna'Āina: www.rapiddirect.com/blog

Waiho i kahi manaʻo

ʻAʻole e paʻiʻia kāu leka uila. Ua hōʻailonaʻia nā mahina i koiʻia *

E nānā i luna

E kiʻi i ka manaʻo ʻōlelo koke

Eʻoluʻolu e hoʻopiha i kāuʻike a e hoʻokaʻaʻike mākou iāʻoe koke.