1. Hōʻikeʻike

C93200, Uaʻikeʻia e like me Liamae 660 Ke lawe nei i ka bronze, he mea nui i hoʻohana nuiʻia e pili ana i nā koho balota i hanaʻia no nā noi e koi ana i ka paleʻana i ke kū'ē a me ka machinibility.

Papaʻia ma lalo alakaʻi-tin bronze alloys, Ua lilo ia i kahi kūlanaʻoihana i nā mea i loaʻa i nā kumulāʻau a me nā lāʻau ma muli o kāna mau mea maikaʻi maikaʻi loa a me nā hana kūpono.

I loko o ka metallirgy, Hoʻopiliʻo C93200 i kahi hana koʻikoʻi i nā'āpana i ka hanaʻana ma lalo o nā ukana haʻahaʻa a me nā wikiwiki.

ʻO kona mauʻano ma waena o nā wahi hana e hana nei -ʻoi loa i ka mana o ka wai, Marine, a me nā'ōnaehana mīkini hana-hana i kahi mea nui ma nā mea hanaʻeluaʻelua (OEM) a me ke kua hope.

2. He aha ka c93200 keleawe moly?

C93200, Uaʻikeʻia e like me Liamae 660 lawe mau bronze, he hana kiʻekiʻe i alakaʻiʻia i nā bronze alloy Hoʻohana nuiʻia no nā noi e pili ana i ka Friction, ʻaʻa, a me nā ukana haʻahaʻa.

Ua hana ia no ka manika superior, Hoʻokomoʻiaʻo EMBISDED TOBRIS, a me ke kū'ēʻana, kūikawā i loko o nā wahi lubricated.

Ma kahiʻano maʻamau i kaʻohana Bronze, Ua hoʻomaopopoʻia no kona kaulike o ka ikaika ikaika, ʻO ka hanaʻana o Tribological, a me ke kumukūʻai-kūpono.

C93200 Bronz Busiing
C93200 Bronz Busiing

ʻO C93200 ka mea maʻamau i hanaʻia ma o ʻO nā kaʻina hana e like me ke one, Kesighu, a me ka hoʻomau mauʻana, a ua nui ka hoʻohanaʻana i nā lāʻau, nā mea kanu, Kāhele, a me nā'āpana pā.

ʻO kāna huiʻana a me nā microstructure e hana pono ai i nā mea e pono ai no nā mea hana e hana ai palena palena a i hui pūʻia i kāwiliʻia.

Kinohi

Mua Kaonaʻeha (%) Hana ma alloy
keleawe (Cu) 83.0 - 88.5 Nā Pākuʻi Base Metal; Hāʻawi i nā drctility a me keʻano
Kū (Sno) 6.3 - 7.5 Hoʻohui i ka ikaika, paakiki, a kau pale
Alakaʻi (Pb) 6.0 - 8.0 E hoʻonui i ka machninctional a me nā embeddability
Zinc (Zn) 1.0 - 4.0 Hoʻomaikaʻi i ka wai; ʻO ka mea hāʻawi kālā kālā liʻiliʻi
'Eron (Lia) ≤ 0.25 Kaohiʻana; ʻO ka hao nui e hōʻeha i ka brittleness
Nickel (I) ≤ 0.25 Koho koho; hoʻomaikaʻi i ke kū'ē kū'ē
Maahua ≤ 0.50 (Nui) Palena palena

Nā Kūlana a me nā hoʻolālā

  • Helu helu: C93200
  • SAE PANUI: Liamae 660
  • Nā inoa kālepa maʻamau: Ke lawe nei i ka bronze, 660 Bronze, Liamae 660 Bronze
  • Nā kiko'ī kiko'ī: B505 (mau ka laweʻana), N271 (Hale Kauka), Na B148 (kuhikuhi'inā)
  • ISO: Cusn7pb7zn4

3. Nā Huakaʻi Mechanical o C93200 Chops Alphaloy

C93200 (Liamae 660) kaulanaʻo ke keleawe no kāna nā mea pono maikaʻi loa ʻO ia ka mea kūpono no ka laweʻana a me nā noi e pili ana i lalo o nā ukana haʻahaʻa a me nā wikiwiki.

ʻO ka hana a Alloy kahi hana o kāna mea hoʻonohonoho, moloka, a me ke kāheaʻana.

Hōʻike ia ʻO ka Mancinability maikaʻi, ʻO ka ikaika hōʻeha maikaʻi, and Mālama i keʻano-ʻAʻole i loko o nā wahi libricated.

C93200 e lawe ana i ka bronhe i ka blashing aila
C93200 e lawe ana i ka bronhe i ka blashing aila

ʻO nā mea waiwai nui

Waiwai Waiwai maʻamau Nā memo
Ikaika ikaika 220 - 275 Mpa Hoʻololi me keʻano kūʻai (Sar vs. Kesighu)
Ka ikaika (0.2% Kahiki) 105 - 130 Mpa ʻOi aku ka kiʻekiʻe ma nā'āpana cenrifugal ma keʻano he nui ma muli o keʻano nui
Elongation ma ka wā hoʻomaha 10 - 20% Hōʻike i nā haʻahaʻa haʻahaʻa
Paʻakikī paʻakikī 65 - 85 HB Hiki ke hoʻonui ma hope o ka hanaʻana i ka hana paʻakikī a iʻole ka mālama kino
ʻO ka ikaika e hāʻawi ai i ka ikaika ~ 120 mpa Kūpono no ka laweʻana i nā ukana
Ka ikaika ~ 170 mpa Mea nui i ka hoʻopiliʻana i nā noi pili
Ka ikaika momona ~ 90 mPA (I 10-style) Hoʻokumuʻia ma nā hōʻikeʻo Beam i loko o nā kūlana Lubricated
Modulus olasticity ~ 100 GPA ʻO nā mea elastic elastic elastic ma lalo o ke kaumaha

Markinpalibility

Hōʻikeʻiaʻo C93200 ʻO ka Mancinability maikaʻi, helu pinepine ma 80-90% ua hoʻohālikelikeʻia i ke keleawe kalaʻole (C36000 = 100%).

Ka heleʻana o ke alakaʻi (6-8%) Ua hāʻawi nui i ka mana o Chip, hoʻemiʻia nā mea hana, a me ke kiʻekiʻe kiʻekiʻe e hoʻopau i ka maikaʻi.

Hana kēia iā C93200 i kahi koho koho i kohoʻia ma CNC-Mactiden Bhoding Should a me nā lāʻau hydraulic.

  • Ka helu matchinbility: ~ 85%
  • ʻO nā mea pono kūpono: HUSS a me nā mea hana kaʻa kaʻa
  • ʻO ka hoʻopau maʻamau: 0.8 - 1.6 μM RA me nā uku hānai kūpono

4. Nā lako kino o c93200 keleawe alloy

C93200, or see 660 Ke lawe nei i ka bronze, hōʻike i kahi hoʻonohonoho kūpono kūpono o Nā Pūnaewele Pūnaewele e kūpono i nā noi kūpono e pili ana i nā noi Ke neʻe nei, Ke Kauka Kauka, a me ke kaumaha kino.

ʻO kēia mau hiʻohiʻona pilikino e hāʻawi pololei i ka pono o ka alloy, Bussings, a me nā'āpana hydraulic -ʻoi loa kūlohelohe, ʻO ke kūpaʻa kūpono, a me ka lawe koiʻia.

C93200 bronze chionsing
C93200 bronze chionsing

ʻO nā waiwai pilikino

Waiwai Waiwai maʻamau Nā'ōlelo'ōlelo
Huakai 8.8 g / cm³ (8800 kg / m³) Hāʻawi i ka nui a me ka hoʻomauʻana i nā mea hana
Hoʻohemo melū 930 - 1020 ° C Liʻiliʻi ma lalo o ke keleawe maʻemaʻe ma muli o ke alakaʻi a me ka tin
Ka HōʻaʻO Kokua ~ 5 58-70 w / m · k Haʻahaʻa ma mua o ke keleawe maʻemaʻe akā lawa no ka weheʻana i ka wela
ʻO ka mana wela ~ 0.38 j / g · g Pili i ka paneʻana i nā'ōlelo noi wikiwiki
Ka maikaʻi o ka hoʻonuiʻana i ka ~ 18.5 × 10⁻⁶ / k Mea nui i ka press-kūpono a me nā hui kiʻekiʻe
Mea kūʻai uila ~ 10-15% IACS ʻAʻole maʻamau i hoʻohana pinepineʻia ma nā kamepiula uila
Modulus olasticity ~ 100 GPA E hōʻike i ka paʻakikī ma lalo o ka ukana
TRUFMUSIKI ~ 2.4 × 10 10⁻⁵ m² / s E hōʻike ana i ka helu o ka wela e pālahalaha i loko o ka waihona
ʻO ka laulā o Poisson ~ 0.31 E wehewehe i ka hoʻonuiʻana ma lalo o ke kaumaha me ke kaumahaʻole

Holo Maʻaleʻa

Mālamaʻo C93200 i keʻano kūlike ma luna o A ka hana ākea ākea ākea, maʻamau a hiki i 205° C (400° F) I ka lawelawe mau, Ke kūpono nei i kūpono no nā'āpana koʻikoʻi.

Kū ponoʻole

ʻO ka hoʻolahaʻana o ka allolo haʻahaʻa haʻahaʻa I ka wā hoʻomaha (~ 1.2-1.5%) a me kahi microstructure uniform i ka wā e hoʻolei ponoʻia.

5. Nā hiʻohiʻona kiʻi o ka C93200 Chopi

C93200 COPPER ALYOR, kaulana loa e like me Sae 660 Ke lawe nei i ka bronze, ua manaʻo nuiʻia ma ka hana hana no kāna ʻO ka Castability maikaʻi loa, ʻO ke kūpaʻaʻo Dimedonal, and Hoʻoponopono i nāʻano hana kūʻai likeʻole.

Kona hui kūʻokoʻa-maʻamau i ka heleʻana o ke alakaʻi (Pb), kū (Sno), a me zinc (Zn)-ʻOiʻo ia i makemake nuiʻia no ka mālamaʻana i nāʻano paʻakikī i ka wā e mālama ana i ka maikaʻi a me ke kani kūloko.

C93200 Bronz BURTY Calting Calting
C93200 Bronz BURTY Calting Calting

ʻO nā hiʻohiʻona helu kī

Hale kūʻai C93200 COPPER ALYOR Nā'ōlelo'ōlelo
Kaulikeia High Alakaʻi a alakaʻi a hoʻomaikaʻi i nā kahe kīwī molten
ʻO ka helu shrink ~ 1.2 - 1.5% Aeʻae i ka uku uku kūpono
Lokole Haole Hoʻohaʻahaʻa ʻO ke kū'ē maikaʻi e pale i ka wā o ka hoʻoponoponoʻana
Malama Tendency Tendency Loli Kāohiʻia ma o ka gating a me ka degosing
ʻO nā wahi noho Loli Koi aku i ka mālama ponoʻana a me nā lāʻau lapaʻau
Matchinability ma hope o ka hoʻoleiʻana Kūpono E like me ka mea i hoʻopaʻaʻia e nā microstructure i kaʻokiʻana a hoʻopau
Kālamalama High (Ma ke kenekulia a me ka hoʻomau mauʻana) ʻO keʻano o keʻano kūpono i nāʻano koʻikoʻi

Nā hana maʻamau no C93200

Ke Kūleʻa Kūlana Kūpono no c93200 Nā noi maʻamau
Sand cread Maikaʻi loa no nāʻano nui a paʻakikī Nā Hale Hōʻikeʻike, Gear Blanks, nā mea nui nui
ʻO Centricugual kāhea Kūpono no nā'āpana cylindrical; Minor Poossity ʻO nā lāʻau kiʻekiʻe kiʻekiʻe, make mau nō pīnō'ī, liners
Hoolei Make 'Ōula (Hiki i ke alakaʻi alakaʻi ke hōʻole i ka make) Liʻiliʻi, nā mea kiʻekiʻe kiʻekiʻe
Ke hoʻomau mau nei Maikaʻi no ka hoʻihoʻiʻana a me ka palaoa nui Nā'āpana likeʻole e koi ana i ka hoʻopau maikaʻiʻana
Ke hoʻomau nei Makemakeʻia no nā hiʻohiʻona stock (ʻO nā Roos, tuku) Nā Kūlana Machined, bar stock no nā mea hana maʻamau

6. E kāʻei i ke kū'ē a me keʻano hana

C93200's Tribological High Stiffity:

  • ʻO ka Lubrication iho: Nā mea i alakaʻiʻia (5-20 μm in conimeter) E hana e like me ka "micro-micrings", ʻO ka pīpī ma nā wahi papahele e hana ai i kahi kiʻiʻoniʻoni haʻahaʻa haʻahaʻa.
    Hoʻemi kēia i ka pono o ka friction i 0.15-0.20 (vsa. 0.6-0.8 no ke kila kila-on-kila).
  • Nā palena PV: Palekana no ka hoʻomau mauʻana ma PV (Meme kaomi × Lumia) nā waiwai a hiki i 1.5 Mpa · m / s (E.g., NA LOA HOOPONOPONO).
    ʻOi aku ka nui o kēia paepae i ke alakaʻiʻana i ke alakaʻi (Ke alakaʻi i nā leo ma 327 ° C), ʻO ka lole hana.
  • E hoʻohana i ka mīkini: Hōʻike i ka lole a me ka lole, Me ka liʻiliʻi o nā kānaka he nui-koʻikoʻi no nā wahi maʻemaʻe e like me ka hoʻomaʻamaʻaʻana o ka meaʻai (me nā mea hoʻokele alakaʻi alakaʻi).

I nā hōʻike hōʻike, C93200 Bushsings i loko o nā mīkini hana agricultural 10,000+ hola ma lalo o ka lubrication palupalu, Kālā Bighoming (C36000) e 3.

7. Kūwaho kūwaho o c93200 keleawe moly

Hāʻawiʻo C93200 i ka paleʻana i ka corrosition corrosion i loko o nā wahi kīnāʻole:

  • Hōʻike Inshothshor: Hana i kahi patina pale (ʻO ka carbonate maʻamau) i nā wahi'āina, Me nā uku corrosioni <0.01 MM / makahiki-kūpono no nā mīkini hana waho.
  • Weʻai: Kū i ka corrosio ma ka wai 6-8 wai (E.g., 'ōnaehana Papa, ʻO nā pimps hou) me nā uku <0.02 MM / makahiki.
  • Ka paʻakai / chrides: Uaʻoi aku ka nui o nā uku pale 0.1 MM / makahiki i loko o ke kai (35,000 PPM CL⁻ bIND) Ma muli o ke koiʻana o ke alakaʻi i ka hoʻopihaʻana a me ka palena o ka tin e hana ai i kahi hana pale pale pale.
  • Kinopa: E hoʻokaʻawale i nā aila, Kupu, a me ka alkalis alkalis (E.g., 10% Naoh at 25 ° C.) Akāʻo nā huiʻana e wikiwiki i nā acids (E.g., 5% sulfuric acid: 1.2 MM / makahiki).

Nā pale palekana: Kālai Epyore, TIN pākuʻi, a iʻole chromate hoʻololi i nā coatistor e hoʻonui i ke ola lawelawe i ka wai i ka hoʻohaʻahaʻa a iʻole nā kahakai ma ka 2-3 ×.

8. Nā noi o c93200 keleawe moly

C93200's Vrestility Spans i nāʻoihana e koi ana i nā'āpana kū ponoʻana:

C93200 bronze pump studeller
C93200 bronze pump studeller
  • Kāhele & Bussings: ʻO nā countershaft CranMothaft Choices (hui mele 660 Nā kiko'ī), Kāpenaehana kikowaenaʻokoʻa, a me nā kaʻa kaʻa kaʻa uila-level-left-lubrication e hōʻemi i ka mālama mālama.
  • Nā'āpana Hydraulic: Nā lāʻau lāʻau, ʻO nā paila i hana i nā mokuahi, a me nā cylinder liners-resingist e pale ana mai nā wai hydraulic (E.g., kahea maikaʻi mineral, wai-glycol mume).
  • Kaʻa kaʻa: Nā apo i hoʻounaʻia, ʻO ka hoʻokele kālāʻana, a me ka hoʻopiʻiʻana i nā helu pivot pivot 100,000+ Km o ka lawelawe ma nā kaʻa kaʻa.
  • Marine (Weʻai): ʻO nā pahu o ka'āina ma loko, Nā'āpana pā, a me nā hatch hinges-pale aku i ka hōʻikeʻana i ke kai.
  • Peopleʻoihana: ʻO nā mea hoʻokūkū hoʻokūkū, E kaomi i nā alakaʻi alakaʻi, a me nā mea hana agricultural pedy, lepo, a me nā mea kolohe.

9. Advent of C93200 Chopper Alphaloy

  • ʻO ka Lubrication iho: E alakaʻi i nā'āpana e hoʻopau i ka pono no ka hoʻomau mauʻana i nā noi haʻahaʻa haʻahaʻa, ʻO ka hōʻemiʻana i nā uku Downtime a me nā kumukūʻai hana.
  • ʻO ka machnitionalʻokoʻa: 80-90% helu helu inoa inoa (vsa. 30% No C95400 aluminum bronze) ʻokiʻia ka hana hana ma ka 20-30% a hoʻopau i ke ola pono.
  • Kumaikalua: 15-20% elongation esorbs shock shock, hōʻemi i ka hikiʻole ke pilikia i ka mīkini kaumaha (E.g., Nā mea hana kūkulu).
  • Kumukūʻai-kūpono: 30-40% cheaper ma mua o ke keleawe alumini (C95400) No nā hana haʻahaʻa haʻahaʻa, ʻO ka maikaʻi no ka hana kiʻekiʻe-Volume High.
  • Whola: Nā Adapts i nā hana e kau ana i nā hana, hiki i nā geomex paʻakikīʻole me kaʻole o ka hanaʻana i ka heluʻana-e hōʻemi ana i ka helu helu helu.

10. Nā palena o C93200 Chops Alphaloy

  • Alakaʻi i ka toxicity: Hoʻopaʻaʻia i loko o ka hālāwaiʻaina meaʻai (FDA 21 Cfr 178.3280 nā palena e alakaʻi ai <0.1%) a me nā mea lapaʻau, e koi ana i nā koho koho mua (E.g., C86300 Manganese Bronze) I kēia mau'āpana.
  • Mahameha: Lss 20% o ka ikaika o ka maka ma 150 ° C; ʻaʻole kūpono no nā noi wela kiʻekiʻe (E.g., Nā Hana Hoʻolaha Exehust, ʻO nā mea hana).
  • Paʻakikī paʻakikī: 60-80 e hoʻohana mau i nā palena hb (≥5 mpa) a iʻole ka wikiwiki (≥5 m / s) noi, kahi i makemakeʻia ai nā bronzes alumini.
  • ʻO ka corrosionion maʻamau: ʻAʻole i'ōleloʻia no ke kai, ʻO nā wahi ACIDIC, a iʻole nā hopena kiʻekiʻe-chrlode (E.g., ʻO ka hoʻolaha paʻakai paʻakai).

11. Hoʻohālikelike hoʻohālikelike me nā bronzes'ē aʻe

C93200 (Liamae 660) ʻO ka laweʻana i ka bronze kekahi o nā mea kūʻai keleawe i hoʻohana nuiʻia ma muli o kāna kaulike maikaʻi loa o ka machinenability, E kāʻei i ke kū'ē, a me ka pā.

Akā naʻe,, I nā noi noi, Hoʻohālikelike pinepineʻia ia i nā alloys'ē aʻe e like me C95400 (ailunimina bronze), C83600 (Keka ulaula ulaula), and C36000 (ʻO ke keleawe manuahi manuahi).

Nā Papa Hoʻolālā: C93200 vs. Nā koho balota'ē aʻe

Waiwai / Alloy C93200 (Liamae 660) C95400 (Ailunimina bronze) C83600 (Keka ulaula ulaula) C36000 (ʻO ke keleawe manuahi manuahi)
Ka Hoʻolālā CU-SN-PB-ZN Cu-Al-Fe-Ni CU-SN-ZN-PB Cu-zn-pb
Ikaika ikaika (Mpa) 200-275 450-700 170-250 345-550
Hālulu (Mau Kanaka Waiwai) 60-80 125-175 50-70 80-100
Markinpalibility Kūpono (80-90%) Loli (30-40%) Maikaʻi loa (60%) Kūpono (90%+)
Ke kū'ē neiʻo Corrosionion Loli Kūpono (esp. Ke wai wai) Maikaʻi loa ʻIlihune i ka maʻalahi
E kāʻei i ke kū'ē Maikaʻi loa Kiʻekiʻe loa Kūpono Loli
Kālā Loli High Loli Hoʻohaʻahaʻa
Nā noi noi Maikaʻi me ka lubrication Maikaʻi loa a iʻole lubricated ʻAʻole kūpono Paʻa
Ka hoʻokaʻawaleʻana Kūpono Kūpono i ka maikaʻi Kūpono ʻAʻole i hoʻokaʻawaleʻia
Hoʻohana maʻamau Kāhele, Bussings ʻO nā pā lāʻau kiʻekiʻe, Pumps Plumbing, Nā Vilves Nā wilipū, KahawaiOli

C93200 vs. C95400 (Ailunimina bronze)

  • Ikaika & Ka lawena i ka hiki: C95400 nui loa i waho c93200 ma ka ikaika o ka maʻi a me ke kāʻeiʻana, e hana ana i kahi kūpono no loa-mokula, nā noi kiʻekiʻe kiʻekiʻe E like me nā mea waiwai a me nā mea kūʻai aku.
  • Ke kū'ē neiʻo Corrosionion: ʻO ka hōʻikeʻo C95400 ke kū'ēʻana i ke kai, chrlodes, a me nā mea kanu, e hana ana i nā mea i makemakeʻia i loko airine and on onfshore nā wahi.
  • Markinpalibility: ʻOiai ka lōʻihi, Uaʻoi aku ka paʻakikī o C95400 i nā mīkini aʻoi aku ka nui o ka uku ma mua o C93200.
  • Hoʻohana kū'a'ā: Koho C93200 No nā kumu kūʻai nui-kumu; Koho C95400 I ka wā e koʻikoʻi ai ka ikaika a me ka paleʻana.

C83600 (Keka ulaula ulaula) vsa. C93200

  • Kālā & Whola: ʻO nā mea a nā alloys e hoʻokaʻawaleʻia, aka, C83600 he cheaper a hoʻohana pinepine i loko nā noi piliʻole e like me nā'āpana a me nā'āpana hoʻonaninani.
  • Hana: Uaʻoi aku ka maikaʻi o C93200 i ke kū'ēʻana i ke kū'ēʻana a me ke kaomiʻana i ka mana, no ka sliding a iʻole nā'āpana'āpana.
  • Hoʻohana kū'a'ā: Koho C83600 No ka uku haʻahaʻa, ʻO Corrosionion-resistant Fittys; hoʻohana C93200 no nā wahi e pono ai i ka lubrication a me ka dimensional kiʻekiʻe.

C93200 vs. C36000 (ʻO ke keleawe manuahi manuahi)

  • Markinpalibility: C36000 ka helu helu helu kiʻekiʻe ma waena o nā mea kūʻai keleawe (>90%), Kūpono no ka wikiwiki kiʻekiʻe e huli ana a me nā'āpana kūpono.
  • Nā Pīkuhi Propertinies: ʻOiai ikaika a me ka pololei, C36000 lacks i ka ʻO nā waiwai a me nā momona momona koiʻia no ka laweʻana i nā papa.
  • Hoʻohana kū'a'ā: Hoʻohana C36000 No nā hana kikowaena, Nā Kākoʻo, a me nā'āpana māmā; hoʻohana C93200 IA MEA lubrication, E kāʻei i ke kū'ē, a me ka pā ke kī.

12. Hopena

C93200 keleawe alloy e noho ana i kahi cornestone o ka hoʻolālāʻoihana no ka ʻO nā noi noi Ma muli o kāna huiʻana o markinpalibility, ʻO ka hoʻomauʻana, a me ke kū'ēʻana.

ʻOiaiʻaʻole pono ke kūpono i nā wahi kiʻekiʻe kiʻekiʻe, Hāʻawi ia i ka hilinaʻi, ʻO ka hana kūpono-maikaʻi i nā mīkini mana nui, lubrication maikaʻi, a he mea nui nā mea paʻa paʻa.

FaqS

Hiki iā C93200 e hoʻohanaʻia me ka lubrication?

ʻAe, I ka uku haʻahaʻa (≤ mPA) a me ka wikiwiki (≤ m / s) noi. ʻO kāna mau alakaʻi alakaʻi i hana me nā lubricies kūloko, hōʻemi i ka friction.

Akā naʻe,, ʻO ka lōʻihi o ka manawa hana i ke ola lawelawe i ke ola kiʻekiʻe ma PV (Meme kaomi × Lumia) Nā hiʻohiʻona.

Is c93200 kūpono no ka hoʻolahaʻana o ke kai?

ʻAʻole. ʻO nā mea iʻike nui aiʻo Seawater i nā mea e pili ana i ka piliʻana i ka corrosiot ma C93200, me nā ukuʻoi aku 0.1 MM / makahiki. No nā noi moana, E hoʻohana i C95400 Aluminum Bronze, e kū ana i ka corrositional kai.

He aha nā mea hou i C93200 no nā noi kiʻekiʻe?

No ka uku nui (≥5 mpa) a iʻole ka wikiwiki (≥5 m / s) noi, Ua makemakeʻo C95400 alumini Bronze, E like me ka hāʻawiʻana iā 2 × i ka ikaika (450-550 mpa) a me nā mea nānā nui.

Hiki iā C93200 mau a iʻole brazed?

ʻAʻole i'ōleloʻiaʻo Welding, E like me ke alakaʻiʻana i keʻano o ke kauʻana i nā wela (≥327 ° C), e kumu ana i ka poosity a me ka brittleness.

Mohaihala (me nā mea hoʻopiʻi kālā kālā) hiki iā ia ke koi akā e koi pono i ka hoʻomākaukauʻana i ka pono e pale aku ai i ke alakaʻiʻana i keʻano o ka hui pūʻana. Hoʻolālā ka mechamical (piulu, kaomi-kūpono) makemakeʻia no ka hui.

Waiho i kahi manaʻo

ʻAʻole e paʻiʻia kāu leka uila. Ua hōʻailonaʻia nā mahina i koiʻia *

E nānā i luna

E kiʻi i ka manaʻo ʻōlelo koke

Eʻoluʻolu e hoʻopiha i kāuʻike a e hoʻokaʻaʻike mākou iāʻoe koke.